JPH0733378Y2 - ナトリウム―硫黄電池 - Google Patents
ナトリウム―硫黄電池Info
- Publication number
- JPH0733378Y2 JPH0733378Y2 JP1988142353U JP14235388U JPH0733378Y2 JP H0733378 Y2 JPH0733378 Y2 JP H0733378Y2 JP 1988142353 U JP1988142353 U JP 1988142353U JP 14235388 U JP14235388 U JP 14235388U JP H0733378 Y2 JPH0733378 Y2 JP H0733378Y2
- Authority
- JP
- Japan
- Prior art keywords
- sodium
- solid electrolyte
- ring
- insulating ceramic
- ceramic ring
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Classifications
-
- Y02E60/12—
Landscapes
- Secondary Cells (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP1988142353U JPH0733378Y2 (ja) | 1988-10-31 | 1988-10-31 | ナトリウム―硫黄電池 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP1988142353U JPH0733378Y2 (ja) | 1988-10-31 | 1988-10-31 | ナトリウム―硫黄電池 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPH0262662U JPH0262662U (de) | 1990-05-10 |
| JPH0733378Y2 true JPH0733378Y2 (ja) | 1995-07-31 |
Family
ID=31408225
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP1988142353U Expired - Lifetime JPH0733378Y2 (ja) | 1988-10-31 | 1988-10-31 | ナトリウム―硫黄電池 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPH0733378Y2 (de) |
Family Cites Families (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS6249866U (de) * | 1985-09-18 | 1987-03-27 | ||
| JPS62295368A (ja) * | 1986-06-13 | 1987-12-22 | Yuasa Battery Co Ltd | ナトリウム−硫黄電池とその製造法 |
-
1988
- 1988-10-31 JP JP1988142353U patent/JPH0733378Y2/ja not_active Expired - Lifetime
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0262662U (de) | 1990-05-10 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US3841912A (en) | Sodium sulfur storage battery | |
| JPH0322028B2 (de) | ||
| WO2012031346A1 (en) | Bi-polar electrochemical cell | |
| JPS6366862A (ja) | ナトリウム−硫黄電池 | |
| JPS5914231B2 (ja) | 密封アルカリ金属バツテリ容器 | |
| JPH0723269B2 (ja) | ナトリウム―硫黄電池における金属製部品とセラミック製部品の結合方法 | |
| KR101353600B1 (ko) | 나트륨 유황 전지 및 그 제조 방법 | |
| JPH02148575A (ja) | ナトリウム−硫黄電池とその接続方法 | |
| JPH02165574A (ja) | ナトリウム‐硫黄電池とその接続方法 | |
| JP4028671B2 (ja) | 熱電池 | |
| JPS6116601Y2 (de) | ||
| JPH0821386B2 (ja) | 扁平形非水液体活物質電池 | |
| JPS6319773A (ja) | ナトリウム−硫黄電池とその製造法 | |
| JPH071735Y2 (ja) | ナトリウム−硫黄電池 | |
| JPH0633647Y2 (ja) | ナトリウム−硫黄電池における絶縁リングと電極容器との結合構造 | |
| JP2633333B2 (ja) | ナトリウム−硫黄電池 | |
| JPH0745885Y2 (ja) | 熱電池 | |
| JP2526285Y2 (ja) | ナトリウム―硫黄電池 | |
| JP3478307B2 (ja) | 熱電池 | |
| JPH07226227A (ja) | 電気化学的蓄電池 | |
| JPH02257576A (ja) | ナトリウム―硫黄電池 | |
| JPS6251149A (ja) | ナトリウム―硫黄電池の製造法 | |
| JPH0675408B2 (ja) | ナトリウム一硫黄電池 | |
| JPH0626135B2 (ja) | ナトリウム−硫黄電池 | |
| JPS5837662U (ja) | 扁平形電池 |