JPH0813166A5 - - Google Patents
Info
- Publication number
- JPH0813166A5 JPH0813166A5 JP6-144208A JP14420894A JPH0813166A5 JP H0813166 A5 JPH0813166 A5 JP H0813166A5 JP 14420894 A JP14420894 A JP 14420894A JP H0813166 A5 JPH0813166 A5 JP H0813166A5
- Authority
- JP
- Japan
- Prior art keywords
- etching solution
- complexing
- complexing agent
- tin
- amendment
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Links
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP14420894A JPH0813166A (ja) | 1994-06-27 | 1994-06-27 | TiNおよびTiのエッチング液 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP14420894A JPH0813166A (ja) | 1994-06-27 | 1994-06-27 | TiNおよびTiのエッチング液 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPH0813166A JPH0813166A (ja) | 1996-01-16 |
| JPH0813166A5 true JPH0813166A5 (mo) | 1999-11-26 |
Family
ID=15356748
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP14420894A Pending JPH0813166A (ja) | 1994-06-27 | 1994-06-27 | TiNおよびTiのエッチング液 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPH0813166A (mo) |
Families Citing this family (14)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| DE10014915B4 (de) * | 2000-03-17 | 2007-08-16 | Infineon Technologies Ag | Verfahren zum Freilegen einer Kontaktfläche |
| JP4535232B2 (ja) * | 2003-11-17 | 2010-09-01 | 三菱瓦斯化学株式会社 | チタンまたはチタン合金のエッチング液 |
| US8300167B2 (en) | 2007-06-14 | 2012-10-30 | Sharp Kabushiki Kaisha | Display panel, display device, and method for manufacturing display panel |
| US8110508B2 (en) | 2007-11-22 | 2012-02-07 | Samsung Electronics Co., Ltd. | Method of forming a bump structure using an etching composition for an under bump metallurgy layer |
| TW201113962A (en) | 2009-10-14 | 2011-04-16 | Advanced Semiconductor Eng | Chip having metal pillar structure |
| TWI445147B (zh) | 2009-10-14 | 2014-07-11 | 日月光半導體製造股份有限公司 | 半導體元件 |
| US8884443B2 (en) | 2012-07-05 | 2014-11-11 | Advanced Semiconductor Engineering, Inc. | Substrate for semiconductor package and process for manufacturing |
| JP6009971B2 (ja) | 2012-11-16 | 2016-10-19 | 株式会社東芝 | 半導体記憶装置及びその製造方法 |
| KR102877724B1 (ko) | 2020-02-05 | 2025-10-29 | 삼성전자주식회사 | 식각 조성물 및 이를 이용한 반도체 소자의 제조 방법 |
| US12308249B2 (en) | 2020-04-14 | 2025-05-20 | Mitsubishi Gas Chemical Company, Inc. | Etching liquid for titanium and/or titanium alloy, method for etching titanium and/or titanium alloy with use of said etching liquid, and method for producing substrate with use of said etching liquid |
| CN115261863B (zh) * | 2022-08-02 | 2024-03-26 | 扬州国宇电子有限公司 | 一种用于快恢复二极管的金属颗粒腐蚀液及金属腐蚀方法 |
| CN116162932B (zh) * | 2022-12-12 | 2024-08-23 | 江苏中德电子材料科技有限公司 | 一种集成电路用铜钛蚀刻液及其制备方法 |
| CN117448823A (zh) * | 2023-07-06 | 2024-01-26 | 江西斯坦德电极科技有限公司 | 一种钛阳极表面处理蚀刻液 |
| JPWO2025141873A1 (mo) | 2023-12-28 | 2025-07-03 |
-
1994
- 1994-06-27 JP JP14420894A patent/JPH0813166A/ja active Pending
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| TW301762B (en) | Pre-thermal treatment cleaning process | |
| JPH07297163A5 (mo) | ||
| JP2000091289A5 (mo) | ||
| WO2003100844B1 (en) | Method for forming silicon dioxide film on silicon substrate, method for forming oxide film on semiconductor substrate, and method for producing semiconductor device | |
| JP3649771B2 (ja) | 洗浄方法 | |
| JPH0813166A (ja) | TiNおよびTiのエッチング液 | |
| JPH11131093A5 (mo) | ||
| JPH08264498A (ja) | シリコンウエーハの清浄化方法 | |
| JPH0831781A5 (mo) | ||
| CN101515539B (zh) | 重掺杂锑硅片的减薄腐蚀方法 | |
| TW496099B (en) | Removal of post-RIE polymer on Al/Cu metal line | |
| JPH08107144A5 (mo) | ||
| US4040893A (en) | Method of selective etching of materials utilizing masks of binary silicate glasses | |
| JP3689871B2 (ja) | 半導体基板用アルカリ性洗浄液 | |
| JPS6125211B2 (mo) | ||
| JPH10230282A5 (mo) | ||
| JP2005146358A (ja) | チタンまたはチタン合金のエッチング液 | |
| JPH09134899A5 (mo) | ||
| JPH05315339A (ja) | 半導体装置におけるバンプ電極形成方法 | |
| JPH03218015A (ja) | 半導体基板の洗浄液及び半導体装置の製造方法 | |
| JP2005203467A (ja) | エッチング用組成物 | |
| JPH04263086A (ja) | シリコン基板のエッチング方法 | |
| JP2001244228A (ja) | 半導体基板の洗浄液及び洗浄方法 | |
| JP2004327969A (ja) | 半導体ウエハの接着前表面処理 | |
| JP2002275667A5 (mo) |