JPH1095861A5 JP1997157832A JP15783297A JPH1095861A5 JP H1095861 A5 JPH1095861 A5 JP H1095861A5 JP 1997157832 A JP1997157832 A JP 1997157832A JP 15783297 A JP15783297 A JP 15783297A JP H1095861 A5 JPH1095861 A5 JP H1095861A5
Authority
JP
Japan
Prior art keywords
cellulose acetate
film
thickness
converted
acetate film
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP1997157832A
Other languages
English (en)
Other versions
JPH1095861A (ja
JP3727754B2 (ja
Filing date
Publication date
Application filed filed Critical
Priority to JP15783297A priority Critical patent/JP3727754B2/ja
Priority claimed from JP15783297A external-priority patent/JP3727754B2/ja
Publication of JPH1095861A publication Critical patent/JPH1095861A/ja
Publication of JPH1095861A5 publication Critical patent/JPH1095861A5/ja
Application granted granted Critical
Publication of JP3727754B2 publication Critical patent/JP3727754B2/ja
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Links

Description

【発明の名称】セルロースアセテートフイルムおよび偏光板保護膜
【0005】
【発明が解決しようとする課題】
従来の通常のソルベントキャスト法により製造するセルロースアセテートフイルムでは、光学的性質や物性の改良が既に限界に近づいている。従来の方法とは全く異なるメルトキャスト法も提案されているが、それにより得られたフイルムは、従来のソルベントキャスト法により製造したフイルムよりも、光学的性質や物性が劣っていた。
本発明の目的は、従来の方法では製造することができなかった、優れた光学的性質や物性を有するセルロースアセテートフイルムおよび偏光板保護膜を提供することである。
【0006】
【課題を解決するための手段】
本発明の目的は、下記(1)〜(7)のセルロースアセテートフイルムおよび下記(8)の偏光板保護膜により達成された。
(1)58.0乃至62.5%の平均酢化度を有し、80μmの厚さに換算したヘイズが0.4%以下であるセルロースアセテートフイルム。
(2)58.0乃至62.5%の平均酢化度を有し、80μmの厚さに換算した引裂強度が20g以上であるセルロースアセテートフイルム。
(3)58.0乃至62.5%の平均酢化度を有し、80μmの厚さに換算したヘイズが0.4%以下であり、かつ80μmの厚さに換算した引裂強度が20g以上であるセルロースアセテートフイルム。
(4)劣化防止剤を含む(1)乃至(3)のいずれか一つに記載のセルロースアセテートフイルム。
(5)セルロースアセテートを有機溶媒で膨潤させた膨潤混合物を、−100乃至−10℃に冷却してから0乃至120℃に加温して得られたセルロースアセテートの有機溶媒溶液を、支持体上に塗布して得られた(1)乃至(3)のいずれか一つに記載のセルロースアセテートフイルム。
(6)有機溶媒が、酢酸メチルを50重量%以上含む(5)に記載のセルロースアセテートフイルム。
(7)反射防止処理が実施されている(1)乃至(3)のいずれか一つに記載のセルロースアセテートフイルム。
(8)上記(1)乃至(7)のいずれか一つに記載のセルロースアセテートフイルムからなる偏光板保護膜。

Claims (8)

  1. 58.0乃至62.5%の平均酢化度を有し、80μmの厚さに換算したヘイズが0.4%以下であるセルロースアセテートフイルム。
  2. 58.0乃至62.5%の平均酢化度を有し、80μmの厚さに換算した引裂強度が20g以上であるセルロースアセテートフイルム。
  3. 58.0乃至62.5%の平均酢化度を有し、80μmの厚さに換算したヘイズが0.4%以下であり、かつ80μmの厚さに換算した引裂強度が20g以上であるセルロースアセテートフイルム。
  4. 劣化防止剤を含む請求項1乃至3のいずれか一項に記載のセルロースアセテートフイルム。
  5. セルロースアセテートを有機溶媒で膨潤させた膨潤混合物を、−100乃至−10℃に冷却してから0乃至120℃に加温して得られたセルロースアセテートの有機溶媒溶液を、支持体上に塗布して得られた請求項1乃至3のいずれか一項に記載のセルロースアセテートフイルム。
  6. 有機溶媒が、酢酸メチルを50重量%以上含む請求項5に記載のセルロースアセテートフイルム。
  7. 反射防止処理が実施されている請求項1乃至3のいずれか一項に記載のセルロースアセテートフイルム。
  8. 請求項1乃至7のいずれか一項に記載のセルロースアセテートフイルムからなる偏光板保護膜。
JP15783297A 1996-07-30 1997-05-29 セルロースアセテートフイルムおよび偏光板保護膜 Expired - Lifetime JP3727754B2 (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP15783297A JP3727754B2 (ja) 1996-07-30 1997-05-29 セルロースアセテートフイルムおよび偏光板保護膜

Applications Claiming Priority (3)

Application Number Priority Date Filing Date Title
JP8-216773 1996-07-30
JP21677396 1996-07-30
JP15783297A JP3727754B2 (ja) 1996-07-30 1997-05-29 セルロースアセテートフイルムおよび偏光板保護膜

Publications (3)

Publication Number Publication Date
JPH1095861A JPH1095861A (ja) 1998-04-14
JPH1095861A5 true JPH1095861A5 (ja) 2004-09-24
JP3727754B2 JP3727754B2 (ja) 2005-12-14

Family

ID=26485144

Family Applications (1)

Application Number Title Priority Date Filing Date
JP15783297A Expired - Lifetime JP3727754B2 (ja) 1996-07-30 1997-05-29 セルロースアセテートフイルムおよび偏光板保護膜

Country Status (1)

Country Link
JP (1) JP3727754B2 (ja)

Families Citing this family (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP4081849B2 (ja) * 1998-04-28 2008-04-30 コニカミノルタホールディングス株式会社 セルロースアシレート溶液の調製方法、セルロースアシレートフィルムの製造方法
JP4797216B2 (ja) * 1999-03-05 2011-10-19 コニカミノルタホールディングス株式会社 ポリマー溶液の調製方法、ポリマーフィルムの製造方法及びポリマーフィルム
JP4534290B2 (ja) * 2000-02-16 2010-09-01 コニカミノルタホールディングス株式会社 光学用フィルムの製造方法
US20090142515A1 (en) 2005-12-21 2009-06-04 Kazuaki Nakamura Cellulose Ester Film, Process for Producing Cellulose Ester Film, Optical Film, Polarization Plate and Liquid Crystal Display Unit
JP4777391B2 (ja) * 2008-06-17 2011-09-21 富士フイルム株式会社 光学用フィルム

Similar Documents

Publication Publication Date Title
JPH115851A5 (ja)
JP4686846B2 (ja) 偏光板用保護フィルム及びそれを用いた偏光板並びに表示装置
US8961845B2 (en) Optical compensation film, and polarizing plate and liquid crystal display employing the same
EP0889080A4 (ja)
JPH0996722A (ja) 偏光板保護膜
EP0483380A4 (en) Processes for synthesizing cyclodextrin polymer and producing cyclodextrin film
JP2001091743A (ja) 位相差板および円偏光板
JP2003012859A (ja) セルロースエステルフィルム、偏光板用保護フィルム及び偏光板
TW201035213A (en) Mixed cellulose ester films having +C plate and -A plate optical properties
AU4538696A (en) Crosslinked tinted polymers
JP6200868B2 (ja) 光学フィルムの製造方法
JPS6040137A (ja) フツ化ビニリデン共重合体フイルム
JPH1095861A5 (ja)
JP5493285B2 (ja) 光学フィルム
JPS6139890B2 (ja)
KR20080029834A (ko) 노르보르넨계 폴리머, 필름, 편광판 및 액정 표시 장치
JP5626347B2 (ja) 光学フィルム用ドープの製造方法、光学フィルムの製造方法、光学フィルム、偏光板、及び液晶表示装置
JP5614450B2 (ja) 光学フィルム用ドープの製造方法、光学フィルムの製造方法、光学フィルム、偏光板、及び液晶表示装置
JP5733066B2 (ja) 光学フィルム及び偏光板
JP2017129852A (ja) 光学補償フィルムおよびその製造方法
JP2018171913A (ja) 透明フィルム及び農業用透明フィルム
JPS6023125B2 (ja) セルロ−スエ−テル皮膜の改質方法
JP2000154278A (ja) 樹脂ブレンド溶液および光拡散フィルム
JP4378739B2 (ja) 偏光板の製造法
JP2009298950A (ja) セルロースアシレートフィルム、及びその用途