JPH11268971A5 - - Google Patents

Info

Publication number
JPH11268971A5
JPH11268971A5 JP1998094048A JP9404898A JPH11268971A5 JP H11268971 A5 JPH11268971 A5 JP H11268971A5 JP 1998094048 A JP1998094048 A JP 1998094048A JP 9404898 A JP9404898 A JP 9404898A JP H11268971 A5 JPH11268971 A5 JP H11268971A5
Authority
JP
Japan
Prior art keywords
particle size
less
maximum particle
quicklime
slurry
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP1998094048A
Other languages
English (en)
Other versions
JPH11268971A (ja
Filing date
Publication date
Application filed filed Critical
Priority to JP9404898A priority Critical patent/JPH11268971A/ja
Priority claimed from JP9404898A external-priority patent/JPH11268971A/ja
Publication of JPH11268971A publication Critical patent/JPH11268971A/ja
Publication of JPH11268971A5 publication Critical patent/JPH11268971A5/ja
Pending legal-status Critical Current

Description

【0012】
【発明の実施の形態】
以下、本発明の実施例を説明する。スラリーの各原料の配合比は、別紙の表1の通り一定とし、珪石の最大粒径を変えて製造した半可塑性体の引っ張り強度、硬化速度、切断可能時間、ダメージの発生状況を比較した結果を別紙の表2に示す。なお、使用したセメントのブレーン値は3000〜3500cm/g程度で、粒径が45μm以上は5〜15%であり、生石灰の粒径が45μm以上は5%以下、また工程繰り返し品の最大粒径は700μm以下である。
JP9404898A 1998-03-23 1998-03-23 Alcパネルの製造方法 Pending JPH11268971A (ja)