JPH1128582A5 - - Google Patents

Info

Publication number
JPH1128582A5
JPH1128582A5 JP1997181252A JP18125297A JPH1128582A5 JP H1128582 A5 JPH1128582 A5 JP H1128582A5 JP 1997181252 A JP1997181252 A JP 1997181252A JP 18125297 A JP18125297 A JP 18125297A JP H1128582 A5 JPH1128582 A5 JP H1128582A5
Authority
JP
Japan
Prior art keywords
joining
friction stir
joining members
stir welding
probe
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP1997181252A
Other languages
English (en)
Other versions
JP4008535B2 (ja
JPH1128582A (ja
Filing date
Publication date
Application filed filed Critical
Priority to JP18125297A priority Critical patent/JP4008535B2/ja
Priority claimed from JP18125297A external-priority patent/JP4008535B2/ja
Publication of JPH1128582A publication Critical patent/JPH1128582A/ja
Publication of JPH1128582A5 publication Critical patent/JPH1128582A5/ja
Application granted granted Critical
Publication of JP4008535B2 publication Critical patent/JP4008535B2/ja
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Links

Claims (12)

  1. 2個の接合部材(1)(2)の突合せ部(3)又は重合せ部に回転するプローブ(12)を挿入し、プローブとの接触部を摩擦熱にて軟化させ撹拌しながら、プローブ挿入状態で、プローブ(12)を突合せ部又は重合せ部に沿って移動させ、あるいはプローブ(12)が順次突合せ部(3)又は重合せ部を通過するように接合部材(1)(2)を移動させることにより、接合部材(1)(2)の突合せ接合又は重ね接合を行うものとなされた摩擦撹拌接合装置であって、
    前記プローブ(12)により接合された接合部(4)を加圧する矯正ローラ(50)が設けられていることを特徴とする摩擦撹拌接合装置。
  2. 上記矯正ローラは、加圧機構を備えた回転自在なローラである請求項1に記載の摩擦撹拌接合装置。
  3. 前記矯正ローラは、上下一対の円柱状ローラであり、互いに両接合部材(1)(2)の平板部(1a)(2a)の厚さ方向に対向する態様にして配置されていることを特徴とする請求項1または2に記載の摩擦撹拌接合装置。
  4. 前記矯正ローラは、両者の隙間が平板部(1a)(2a)の厚さより若干小さく設定され、上下矯正ローラ(50)(51)間に通される両接合部材(1)(2)を軽く圧延し、両接合部材(1)(2)を接合部(4)において矯正して平坦状にしうるものとなされていることを特徴とする請求項3に記載の摩擦撹拌接合装置。
  5. 両接合部材(1)(2)の移動方向における前記上矯正ローラ(50)の後方近傍に、冷却装置の冷却媒体噴射用ノズル(60)が、その噴射口を接合部(4)に向ける態様にして固定配置されている請求項1ないし4のいずれか1に記載の摩擦撹拌接合装置。
  6. 2個の接合部材(1)(2)の突合せ部(3)又は重合せ部に回転するプローブ(12)を挿入し、プローブとの接触部を摩擦熱にて軟化させ撹拌しながら、プローブ挿入状態で、プローブ(12)を突合せ部又は重合せ部に沿って移動させ、あるいはプローブ(12)が順次突合せ部(3)又は重合せ部を通過するように接合部材(1)(2)を移動させることにより、接合部材(1)(2)の突合せ接合又は重ね接合を行うものとなされた摩擦撹拌接合方法であって、前記プローブ(12)により接合された接合部(4)を矯正ローラにより加圧することを特徴とする摩擦撹拌接合方法。
  7. 前記矯正ローラによる加圧により接合部の歪みを除去する請求項6に記載の摩擦撹拌接合方法。
  8. 前記矯正ローラは、上下一対の円柱状ローラであり、前記矯正ローラによる加圧は、互いに両接合部材(1)(2)の平板部(1a)(2a)の厚さ方向に対向する態様にして配置された前記上下矯正ローラにより行われることを特徴とする請求項6または7に記載の摩擦撹拌接合方法。
  9. 前記矯正ローラは、両者の隙間が平板部(1a)(2a)の厚さより若干小さく設定され、上下矯正ローラ(50)(51)間に通される両接合部材(1)(2)を軽く圧延し、両接合部材(1)(2)を接合部(4)において矯正して平坦にすることを特徴とする請求項6ないし8のいずれか1に記載の摩擦撹拌接合方法。
  10. 両接合部材(1)(2)の移動方向における前記上矯正ローラ(50)の後方近傍に設置された、冷却装置の冷却媒体噴射用ノズル(60)により、接合部を強制冷却することを特徴とする請求項6ないし9のいずれか1に記載の摩擦撹拌接合方法。
  11. 2個の接合部材の相互突合せ部に厚肉部を形成した接合部材を用いて接合し、接合部をローラにより加圧する請求項6ないし10のいずれか1に記載の摩擦撹拌接合方法。
  12. 請求項6ないし11のいずれか1に記載の摩擦撹拌接合方法により接合された接合品。
JP18125297A 1997-07-07 1997-07-07 摩擦撹拌接合装置及び摩擦撹拌接合方法 Expired - Lifetime JP4008535B2 (ja)