JPS5522407A - Calcination type flux for horizontal submerged arc welding - Google Patents
Calcination type flux for horizontal submerged arc weldingInfo
- Publication number
- JPS5522407A JPS5522407A JP9367978A JP9367978A JPS5522407A JP S5522407 A JPS5522407 A JP S5522407A JP 9367978 A JP9367978 A JP 9367978A JP 9367978 A JP9367978 A JP 9367978A JP S5522407 A JPS5522407 A JP S5522407A
- Authority
- JP
- Japan
- Prior art keywords
- flux
- arc welding
- submerged arc
- welding metal
- type flux
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
PURPOSE:The above mentioned flux, composed of a fixed composition containing more than one kind of CaF2, BaF2, NaF, AlF3, MgF2 and Al or Al and Si as deoxidizer, decreasing oxygen in welding metal, improving mechanical property and preventing defect generation. CONSTITUTION:The above mentioned flux is contained 20 - 80% of total quantity of more than one kind of CaF2, BaF2, NgF, AlF3 and MaF2 against total quantity of the flux and Al or both Al and Si as deoxidizer, within the limits of 2,5% <=Al+0.5Si<=5.5%, Si<=4%. The above flux is used combining with welding wire composed of Ni base alloy and containing quantity of oxygen in welding metal is remarkably decreased and also, welding metal having superior mechanical property and no inner defect, is formed.
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP9367978A JPS5944959B2 (en) | 1978-08-02 | 1978-08-02 | Sintered flux for horizontal submerged arc welding |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP9367978A JPS5944959B2 (en) | 1978-08-02 | 1978-08-02 | Sintered flux for horizontal submerged arc welding |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS5522407A true JPS5522407A (en) | 1980-02-18 |
| JPS5944959B2 JPS5944959B2 (en) | 1984-11-02 |
Family
ID=14089084
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP9367978A Expired JPS5944959B2 (en) | 1978-08-02 | 1978-08-02 | Sintered flux for horizontal submerged arc welding |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS5944959B2 (en) |
Cited By (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5895608A (en) * | 1981-11-30 | 1983-06-07 | Toshiba Corp | Production of ceramic powder |
| JPS59178196A (en) * | 1983-03-26 | 1984-10-09 | Nippon Steel Corp | Baked flux for three o'clock submerged arc welding |
| JP2011056562A (en) * | 2009-09-11 | 2011-03-24 | Nippon Steel & Sumikin Welding Co Ltd | Method for submerged arc welding of steel for low-temperature service |
| JP2022152690A (en) * | 2021-03-29 | 2022-10-12 | 日鉄溶接工業株式会社 | Submerged arc welding method of steel for low temperature use |
-
1978
- 1978-08-02 JP JP9367978A patent/JPS5944959B2/en not_active Expired
Cited By (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5895608A (en) * | 1981-11-30 | 1983-06-07 | Toshiba Corp | Production of ceramic powder |
| JPS59178196A (en) * | 1983-03-26 | 1984-10-09 | Nippon Steel Corp | Baked flux for three o'clock submerged arc welding |
| JP2011056562A (en) * | 2009-09-11 | 2011-03-24 | Nippon Steel & Sumikin Welding Co Ltd | Method for submerged arc welding of steel for low-temperature service |
| JP2022152690A (en) * | 2021-03-29 | 2022-10-12 | 日鉄溶接工業株式会社 | Submerged arc welding method of steel for low temperature use |
Also Published As
| Publication number | Publication date |
|---|---|
| JPS5944959B2 (en) | 1984-11-02 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| GB1517892A (en) | Welding flux formulation and process for fume reduction | |
| KR910011389A (en) | Flux Filling Wire for Gas Sealed Arc Welding | |
| JPS5772795A (en) | Composite wire for gas shilded arc welding | |
| JPS5674395A (en) | Noncoated electrode wire for arc welding | |
| SE8603900D0 (en) | ELECTRIC FOR LIGHT BACK WELDING | |
| JPS54155139A (en) | Wire for uncovered arc welding | |
| JPS5592290A (en) | Low hydrogen base coated electrode | |
| JPS577396A (en) | Compound wire for gas sealed arc welding | |
| JPS56109192A (en) | Flux-cored wire for vertical and horizontal position arc welding of stainless steel | |
| JPS5462134A (en) | Flux for submerged arc welding of ultralow carbon austenitic stainless steel | |
| SU860972A1 (en) | Electrode coating composition | |
| JPS558326A (en) | Submerged arc welding method of steel for cryogenic temperature service | |
| JPS5762889A (en) | Sintered type flux for submerged arc welding | |
| JPS5592291A (en) | Low hydrogen base coated electrode | |
| JPS57181797A (en) | Composite wire | |
| JPS5411047A (en) | Low hydrogen type coated arc welding electrode | |
| JPS55109593A (en) | Coated electrode | |
| JPS56109193A (en) | Production of extra low hydrogen type coated arc electrode | |
| JPS54127848A (en) | Low hydrogen system coated arc welding electrode | |
| JPS5536007A (en) | Compound wire for automatic and semi-automatic arc welding | |
| JPS57160597A (en) | Manufacture of low-hydrogen type coated electrode | |
| JPS5633196A (en) | High speed submerged arc welding | |
| JPS5691982A (en) | Gas shielded arc welding method | |
| JPS52114514A (en) | Heat treatment type high tensile steel of low nitrogen content, contai ning titanium and having excellent weldability weldability | |
| JPS54134048A (en) | Composite wire for automatic welding |