JPS62210076A - セメント厚型スレ−トの表面塗装法 - Google Patents

セメント厚型スレ−トの表面塗装法

Info

Publication number
JPS62210076A
JPS62210076A JP5297386A JP5297386A JPS62210076A JP S62210076 A JPS62210076 A JP S62210076A JP 5297386 A JP5297386 A JP 5297386A JP 5297386 A JP5297386 A JP 5297386A JP S62210076 A JPS62210076 A JP S62210076A
Authority
JP
Japan
Prior art keywords
slate
carboxylic acid
coated film
styrene
roof tile
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP5297386A
Other languages
English (en)
Inventor
Moriyoshi Matayoshi
又吉 盛義
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to JP5297386A priority Critical patent/JPS62210076A/ja
Publication of JPS62210076A publication Critical patent/JPS62210076A/ja
Pending legal-status Critical Current

Abstract

(57)【要約】本公報は電子出願前の出願データであるた
め要約のデータは記録されません。

Description

【発明の詳細な説明】 「産業上の利用分野」 本発(す」けセメント厚型スレートの表面塗装法に関す
るものである。
「従来の技術」 従来、セメント厚型スレート用塗料(スラリー)では、
スレートの白眉現象のためスレート表面から塗膜が剥離
するため塗装膜の耐候性(長期安定性)、耐亀裂性に乏
しく、そのためスレートの耐水性及び耐老化性を向上す
ることが困難であって、市場性が急速に低下した。
「発明が解決しようとする問題点J 本発明はセメントの水和反応により生成する塩類例えは
水酸化カルシウム、ナトリウム、カリウム、硫酸塩、炭
醗塩等がセメント及び骨材の開−から表面に滲出する所
Wn白華現象を塗装によって抑制し塗膜剥離を防止しよ
うとするものである。
「問題点を解決するための手段」 本発明はスチレンブタジェン系合成ゴムをバインダーと
してカルボン酸及び顔料を混合し、練込水で粘度調整を
行ってこれをスレート表面に吹付けることを特徴とする
セメント厚型スレートの表面塗装法によって構成される
「作用」 従ってスチレンブタジェン系合成ゴムエマルジョン、カ
ルボン酸、顔料及び水との混合物をセメントによるスレ
ート表面に吹付けると同スレート表面に塗膜が形成され
る。そしてスレートの内部から表面に滲出する水和反応
による生成塩類は上記カルボン酸と反応して同塩類を中
和しスレート表面からスレート内部に向って除々に不溶
性のコロイド状物質8を構成し、同物質8けモルタル又
は毛細管を閉塞するため上記白R4現象即ちスレート内
遊離塩類の表面滲出を抑え、又上記コロイド状物質は外
部からの水の滲透を抑制する〇「実施例」 混合機1にセメント40Kp、EMX(スチレンブタジ
ェン系合成ゴムエマルジョン)IOKP、H−2(カル
ボン酸)2Kp、ステンレススチール粉(顔R)2Kp
、アクリル樹脂(又はセラミックス粉)5に2を投入し
水と混合して粘度を調整する0次にこれを100メツシ
スクリンでr過2しその際の粘度は18〜20秒(7オ
ドカツプ)であるOMEプレス3で成形したセメント厚
型スレート4の表面4にプレス直後に上記r過剤を常温
で吹付けて下塗5を1情し、その後これを40〜50℃
で約13時間養生6し、さらに40〜50’Cで吹付け
て上塗り7して仕上げられる。
「効果コ 本発明は上述の方法によったのでスレート内部から表面
に滲出する溶解熱f@塩による所f4スレート表面白華
現象を抑制防止し得てスレート表面の塗膜の剥離現象を
防止し耐久性に富む表面塗装セメントスレートが得られ
る効果がある。
4図面の簡単な説舅 第1図は本発明の表面塗装法によるスレートを示す拡大
縦断面図、第2−は製造工程図である。

Claims (1)

    【特許請求の範囲】
  1. (1)スチレンブタジエン系合成ゴムをバインダーとし
    てカルボン酸及び顔料を混合し、練込水で粘度調整を行
    ってこれをスレート表面に吹付けることを特徴とするセ
    メント厚型スレートの表面塗装法。
JP5297386A 1986-03-10 1986-03-10 セメント厚型スレ−トの表面塗装法 Pending JPS62210076A (ja)