JPS6417876A - Production of metallic pipe coated with tin or tin-base alloy on inside surface - Google Patents
Production of metallic pipe coated with tin or tin-base alloy on inside surfaceInfo
- Publication number
- JPS6417876A JPS6417876A JP62173668A JP17366887A JPS6417876A JP S6417876 A JPS6417876 A JP S6417876A JP 62173668 A JP62173668 A JP 62173668A JP 17366887 A JP17366887 A JP 17366887A JP S6417876 A JPS6417876 A JP S6417876A
- Authority
- JP
- Japan
- Prior art keywords
- tin
- metallic pipe
- alloy
- inside surface
- coating
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
PURPOSE:To easily obtain a metallic pipe coated uniformly with tin (alloy) on the inside surface in a short period of time by inserting a material of a tin system for coating into the metallic pipe and melting and extending the tin (alloy) by high-frequency heating to coat the tin (alloy) over the entire part of the inside surface wall of the metallic pipe, then cooling the metallic pipe. CONSTITUTION:The material consisting of the tin or essentially consisting of the tin for coating (e.g.; tin-zinc alloy) is inserted into the metallic pipe. The metallic pipe is then subjected to the high-frequency heating in an inert gaseous or non-oxidizing atmosphere gas or reducing atmosphere gas to rapidly increase the temp. of the metallic pipe to >=1,000 deg.C and to melt and extend the material for coating, by which the tin (alloy) is coated over the entire inside surface wall of the metallic pipe. The metallic pipe is then cooled as rapidly as possible, by which the metallic pipe coated with the tin (alloy) on the inside surface is obtd. Since the metallic pipe is rapidly heated by the high-frequency heating, the material for coating is melted and extend while the formation of the oxide film on the surface thereof is prevented. The uniform coating is thus obtd.
Priority Applications (5)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP62173668A JP2727184B2 (en) | 1987-07-11 | 1987-07-11 | Method for producing metal tube having inner surface coated with tin or tin-based alloy |
| GB8815996A GB2206899B (en) | 1987-07-11 | 1988-07-05 | Method of manufacturing metal pipes coated with tin or based alloys. |
| DE3823309A DE3823309A1 (en) | 1987-07-11 | 1988-07-09 | METHOD FOR PRODUCING METAL TUBES COATED WITH TIN OR TIN-BASED ALLOYS |
| KR1019880008577A KR910004611B1 (en) | 1987-07-11 | 1988-07-11 | Manufacturing method of metal pipe coated with tin or tin base alloy |
| US07/510,990 US5139814A (en) | 1987-07-11 | 1990-04-19 | Method of manufacturing metal pipes coated with tin or tin based alloys |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP62173668A JP2727184B2 (en) | 1987-07-11 | 1987-07-11 | Method for producing metal tube having inner surface coated with tin or tin-based alloy |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS6417876A true JPS6417876A (en) | 1989-01-20 |
| JP2727184B2 JP2727184B2 (en) | 1998-03-11 |
Family
ID=15964884
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP62173668A Expired - Fee Related JP2727184B2 (en) | 1987-07-11 | 1987-07-11 | Method for producing metal tube having inner surface coated with tin or tin-based alloy |
Country Status (4)
| Country | Link |
|---|---|
| JP (1) | JP2727184B2 (en) |
| KR (1) | KR910004611B1 (en) |
| DE (1) | DE3823309A1 (en) |
| GB (1) | GB2206899B (en) |
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2007278359A (en) * | 2006-04-05 | 2007-10-25 | Kayaba Ind Co Ltd | Worm reducer and electric power steering device |
Families Citing this family (6)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| DE4136038C2 (en) * | 1990-11-02 | 1994-06-16 | Usui Kokusai Sangyo Kk | Welded steel tube with high corrosion resistance of the inner surface and process for its production |
| JP3176405B2 (en) * | 1991-12-02 | 2001-06-18 | 臼井国際産業株式会社 | Welded pipe excellent in corrosion resistance on inner surface and method for producing the same |
| DE4221957C1 (en) * | 1992-07-02 | 1994-01-13 | Mannesmann Ag | Prodn. of thick-walled metal high-pressure pipes with smooth interiors - by alternating cold deformation and thermal treatment stages plus application of ductile non-ferrous metal or alloy to pipe interior |
| DE19710294C2 (en) * | 1997-03-13 | 2001-04-05 | Wieland Werke Ag | Process for the production of a corrosion-resistant pipe |
| DE19710292C2 (en) * | 1997-03-13 | 2001-05-03 | Wieland Werke Ag | Process for the production of a tinned strip |
| WO2002046495A1 (en) * | 2000-12-05 | 2002-06-13 | Euromat Gesellschaft Für Werkstofftechnologie Und Transfer Mbh | Method and material for coating a cavity of a work piece |
Family Cites Families (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| GB238921A (en) * | 1924-04-22 | 1925-08-24 | Daimler Co Ltd | Improvements relating to the coating internally of hollow articles with metal |
| US1660597A (en) * | 1925-06-16 | 1928-02-28 | Ralph H Conkle | Process for treating brass condenser tubes |
| GB1385256A (en) * | 1972-09-22 | 1975-02-26 | Ici Ltd | Coating and bonding of metals |
-
1987
- 1987-07-11 JP JP62173668A patent/JP2727184B2/en not_active Expired - Fee Related
-
1988
- 1988-07-05 GB GB8815996A patent/GB2206899B/en not_active Expired - Lifetime
- 1988-07-09 DE DE3823309A patent/DE3823309A1/en active Granted
- 1988-07-11 KR KR1019880008577A patent/KR910004611B1/en not_active Expired
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2007278359A (en) * | 2006-04-05 | 2007-10-25 | Kayaba Ind Co Ltd | Worm reducer and electric power steering device |
Also Published As
| Publication number | Publication date |
|---|---|
| JP2727184B2 (en) | 1998-03-11 |
| GB2206899B (en) | 1991-12-18 |
| GB8815996D0 (en) | 1988-08-10 |
| KR910004611B1 (en) | 1991-07-08 |
| DE3823309A1 (en) | 1989-01-19 |
| KR890002439A (en) | 1989-04-10 |
| DE3823309C2 (en) | 1990-03-15 |
| GB2206899A (en) | 1989-01-18 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| EP0387107A3 (en) | Method and apparatus for casting a metal | |
| SG47681A1 (en) | Metallic evacuated double-walled vessel and production method therefor | |
| JPS5797606A (en) | Manufacture of amorphous alloy thin belt having extremely low iron loss | |
| MY104399A (en) | A method for the continuous coating of a filiform steel substrate by immersion of this substrate in a bath of molten coating metal. | |
| JPS57155363A (en) | Method of forming surface covering metal layer | |
| EP0311270A3 (en) | Method of applying low gloss nylon coatings | |
| JPS56129696A (en) | Crystal growing apparatus | |
| JPS57188429A (en) | Coating method for optical fiber with metal | |
| EP0601186A4 (en) | Production method for metal cadmium powder. | |
| JPS62112769A (en) | Formation of thermally sprayed film having superior wear and corrosion resistance and durability | |
| JPS574376A (en) | Cementation method of glass | |
| JPS5488843A (en) | Surface treating method for metallic alloy member | |
| JPS5533858A (en) | Production equipment of quenching congelation material | |
| JPS55136552A (en) | Production of broad amorphous metal tape and producing apparatus thereof | |
| JPS5770062A (en) | Method and device for producing amorphous metallic coil | |
| Krivosheev et al. | Determining the Temperature of Film Formation on Synthetic Pig Irons | |
| Bell | Various Ways of Fusing Sprayed Deposits | |
| Psiuk et al. | Procedure for the Production of a Wear-Reducing Layer | |
| JPS5625951A (en) | High permeability alloy sheet | |
| Movchan | Apparatus and Method for Producing Carbide Coatings | |
| JPS6415264A (en) | Device for manufacturing composite metal stock | |
| JPS54145345A (en) | Manufacture of flux coating solder | |
| JPS64461B2 (en) | ||
| JPS57210964A (en) | Hot dipping method using zn-al-sn alloy | |
| Breuer | Process for Refining High-Carbon Ferro-Alloys |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| R250 | Receipt of annual fees |
Free format text: JAPANESE INTERMEDIATE CODE: R250 |
|
| R250 | Receipt of annual fees |
Free format text: JAPANESE INTERMEDIATE CODE: R250 |
|
| LAPS | Cancellation because of no payment of annual fees |