JPS6436717A - 転炉スラグの流出防止方法 - Google Patents

転炉スラグの流出防止方法

Info

Publication number
JPS6436717A
JPS6436717A JP19213687A JP19213687A JPS6436717A JP S6436717 A JPS6436717 A JP S6436717A JP 19213687 A JP19213687 A JP 19213687A JP 19213687 A JP19213687 A JP 19213687A JP S6436717 A JPS6436717 A JP S6436717A
Authority
JP
Japan
Prior art keywords
slag
cao
sio2
converter
molten iron
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP19213687A
Other languages
English (en)
Japanese (ja)
Other versions
JPH0480088B2 (lt
Inventor
敏行 金子
英明 山村
矢倉 重範
三隅 秀幸
長田 修次
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Nippon Steel Corp
Original Assignee
Nippon Steel Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Nippon Steel Corp filed Critical Nippon Steel Corp
Priority to JP19213687A priority Critical patent/JPS6436717A/ja
Publication of JPS6436717A publication Critical patent/JPS6436717A/ja
Publication of JPH0480088B2 publication Critical patent/JPH0480088B2/ja
Granted legal-status Critical Current

Links

Landscapes

  • Carbon Steel Or Casting Steel Manufacturing (AREA)
JP19213687A 1987-07-31 1987-07-31 転炉スラグの流出防止方法 Granted JPS6436717A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP19213687A JPS6436717A (ja) 1987-07-31 1987-07-31 転炉スラグの流出防止方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP19213687A JPS6436717A (ja) 1987-07-31 1987-07-31 転炉スラグの流出防止方法

Publications (2)

Publication Number Publication Date
JPS6436717A true JPS6436717A (ja) 1989-02-07
JPH0480088B2 JPH0480088B2 (lt) 1992-12-17

Family

ID=16286283

Family Applications (1)

Application Number Title Priority Date Filing Date
JP19213687A Granted JPS6436717A (ja) 1987-07-31 1987-07-31 転炉スラグの流出防止方法

Country Status (1)

Country Link
JP (1) JPS6436717A (lt)

Cited By (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPH02213408A (ja) * 1989-02-15 1990-08-24 Nisshin Steel Co Ltd ステンレス鋼の転炉スラグ流出防止方法
WO2012132789A1 (ja) 2011-03-31 2012-10-04 日新製鋼株式会社 ステンレス鋼の製造方法
US11060195B2 (en) 2012-08-14 2021-07-13 Loop Energy Inc. Reactant flow channels for electrolyzer applications

Cited By (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPH02213408A (ja) * 1989-02-15 1990-08-24 Nisshin Steel Co Ltd ステンレス鋼の転炉スラグ流出防止方法
WO2012132789A1 (ja) 2011-03-31 2012-10-04 日新製鋼株式会社 ステンレス鋼の製造方法
CN103476953A (zh) * 2011-03-31 2013-12-25 日新制钢株式会社 不锈钢的制造方法
US11060195B2 (en) 2012-08-14 2021-07-13 Loop Energy Inc. Reactant flow channels for electrolyzer applications

Also Published As

Publication number Publication date
JPH0480088B2 (lt) 1992-12-17

Similar Documents

Publication Publication Date Title
US4586956A (en) Method and agents for producing clean steel
CN112430755A (zh) 矿热炉冶炼普通硅锰合金快速转炼高硅硅锰合金的工艺
CN101294233A (zh) 一种铁水预处理同时脱硅脱锰的方法
CN108118115A (zh) 一种vd流程冶炼高碳铬轴承钢的方法
CN103555886B (zh) 一种含钒铁水冶炼超低硫钢的方法
CN116716450B (zh) 一种低硅钢冶炼方法
CN111074037B (zh) 一种升级富锰渣冶炼产品结构的工艺方法
US5037609A (en) Material for refining steel of multi-purpose application
CA1079072A (en) Arc steelmaking
JP3460595B2 (ja) 極低硫鋼の溶製方法
CN115652184B (zh) 一种aod转炉使用化渣剂冶炼超纯铁素体不锈钢的方法
JP2896839B2 (ja) 溶鋼製造方法
JP2976852B2 (ja) キリング時間を短縮した低硫鋼の製造法
JPH0480088B2 (lt)
JP3158912B2 (ja) ステンレス鋼の精錬方法
JPH05222425A (ja) カルシウム・アルミネートによる溶銑脱硫および脱硫滓の処理方法
JPS58147506A (ja) 溶銑予備処理方法
CN117512262B (zh) 一种lf精炼快速熔渣方法
JP3239722B2 (ja) 溶銑の予備処理方法
KR970005383B1 (ko) 고 실리콘(Si)용선으로 저 인[P]강의 제조방법
JP3736229B2 (ja) 溶銑の処理方法
CN109988884A (zh) 提高钢水浇铸性能的钢的制造方法
JPH11100608A (ja) 溶銑の脱珪・脱硫方法
CN117226060A (zh) 一种防止冷镦钢连铸生产过程中水口结瘤的方法
KR910006007B1 (ko) 용강탈린제