PL396368A1 - Sposób otrzymywania wysokotemperaturowego anhydrytu 1-α CaSO4 - Google Patents
Sposób otrzymywania wysokotemperaturowego anhydrytu 1-α CaSO4Info
- Publication number
- PL396368A1 PL396368A1 PL396368A PL39636811A PL396368A1 PL 396368 A1 PL396368 A1 PL 396368A1 PL 396368 A PL396368 A PL 396368A PL 39636811 A PL39636811 A PL 39636811A PL 396368 A1 PL396368 A1 PL 396368A1
- Authority
- PL
- Poland
- Prior art keywords
- caso4
- weight
- temperature
- anhydrite
- obtaining
- Prior art date
Abstract
Wynalazek rozwiazuje problem wytwarzania wysokotemperaturowego anhydrytu I - ? CaSO4. Sposób polega na tym, ze miesza sie gips naturalny (CaSO4 • 2H2O) lub odpadowy reagips (CaSO4 • 2H2O) powstaly w procesie odsiarczania spalin w ilosci 64-90% wagowych ze zmielonym surowcem wapiennym, zawierajacym weglan wapnia, korzystnie kamieniem wapiennym w ilosci 10-36%, wagowych, po czym mieszanine ta wypala sie w temperaturze 1150-1180°C przez 30 do 90 minut, a nastepnie otrzymany spiek chlodzi sie nie wolniej niz 20°C na minute i miele do pozostalosci na sicie 4900 oczek/cm2 wynoszacej okolo 10% wagowych.
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| PL396368A PL220674B1 (pl) | 2011-09-19 | 2011-09-19 | Sposób otrzymywania wysokotemperaturowego anhydrytu I-α CaSO<sub>4</sub> |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| PL396368A PL220674B1 (pl) | 2011-09-19 | 2011-09-19 | Sposób otrzymywania wysokotemperaturowego anhydrytu I-α CaSO<sub>4</sub> |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| PL396368A1 true PL396368A1 (pl) | 2013-04-02 |
| PL220674B1 PL220674B1 (pl) | 2015-11-30 |
Family
ID=48040787
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| PL396368A PL220674B1 (pl) | 2011-09-19 | 2011-09-19 | Sposób otrzymywania wysokotemperaturowego anhydrytu I-α CaSO<sub>4</sub> |
Country Status (1)
| Country | Link |
|---|---|
| PL (1) | PL220674B1 (pl) |
-
2011
- 2011-09-19 PL PL396368A patent/PL220674B1/pl unknown
Also Published As
| Publication number | Publication date |
|---|---|
| PL220674B1 (pl) | 2015-11-30 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| PH12016500190A1 (en) | Calcuim sulfoaluminate composite binders | |
| EA201491112A1 (ru) | Перколированный муллит и способ его получения | |
| BR112016029622A2 (pt) | concreto não-autoconsolidante de desempenho ultra elevado | |
| MX370716B (es) | Material multifásico sustituto de injerto de hueso. | |
| PL2896605T3 (pl) | Kompozycja gipsowa, zawiesina gipsowa, utwardzony korpus gipsowy, materiał budowlany na bazie gipsu, płyta gipsowa i sposób wytwarzania materiału budowlanego na bazie gipsu | |
| EA201890004A1 (ru) | Способ производства высокореактивного цемента | |
| ES2651012T3 (es) | Nuevo clínker sulfo-belítico dopado con fósforo y procedimiento para su preparación | |
| TR200903373A2 (tr) | Yüksek performanslı çimento ve üretim prosesi | |
| CU20160107A7 (es) | Método para curar un producto de calcinación de yeso | |
| PL2150504T3 (pl) | Sposób wytwarzania półwodzianu alfa siarczanu wapnia z dwuwodzianu siarczanu wapnia | |
| ZA202211636B (en) | Cement-manufacturing plant and process for producing cement clinker | |
| BR112012007213A2 (pt) | método e usina para fabricar cimento | |
| PL396368A1 (pl) | Sposób otrzymywania wysokotemperaturowego anhydrytu 1-α CaSO4 | |
| DK2356083T3 (da) | Fremgangsmåde og anlæg til fremstilling af cementklinker | |
| RU2009103066A (ru) | Сырьевая смесь для получения гипсового вяжущего и изделий на его основе | |
| PL413825A1 (pl) | Aktywatory wiązania cementu dla kompozycji cementowych o opóźnionym czasie wiązania i powiązane sposoby | |
| MX347866B (es) | Proceso para producir concreto duradero en condiciones de ambiente caliente. | |
| PL388711A1 (pl) | Granulat wspomagający uprawę roślin i sposób jego wytwarzania | |
| CN104478312A (zh) | 一种承重墙专用节能保温一体化砌块 | |
| EA201500853A1 (ru) | Обработанные при низких температурах сульфаты кальция для быстротвердеющих цементов и общего применения | |
| IN2013MU04002A (pl) | ||
| PL398082A1 (pl) | Mineralno-organiczny preparat paszowy i sposób wytwarzania mineralno-organicznego preparatu paszowego | |
| LV14448A (lv) | Korozijiztur&imacr;gs betons uz &#x123;ip&scaron;a un portlandcementa saistvielas b&amacr;zes | |
| Fridrichová et al. | FBC-Ash as a Substitute of Part Material Raw during Production of Portland Cement | |
| PL411375A1 (pl) | Sposób wytwarzania skonsolidowanych agrokompozytów granulowanych |