PL414098A1 - Method for producing paraffin emulsion - Google Patents

Method for producing paraffin emulsion

Info

Publication number
PL414098A1
PL414098A1 PL414098A PL41409815A PL414098A1 PL 414098 A1 PL414098 A1 PL 414098A1 PL 414098 A PL414098 A PL 414098A PL 41409815 A PL41409815 A PL 41409815A PL 414098 A1 PL414098 A1 PL 414098A1
Authority
PL
Poland
Prior art keywords
parts
weight
reactor
homogenization
stage
Prior art date
Application number
PL414098A
Other languages
Polish (pl)
Other versions
PL228523B1 (en
Inventor
Jan Gniady
Jolanta Iłowska
Bartłomiej Bereska
Michał Szmatoła
Rafał Grabowski
Bronisław Dejnega
Julia Woch
Jolanta Bubicz
Witold Haas
Renata Kubica
Renata Fiszer
Izabela Robak
Grzegorz Kubosz
Iwona Witkowska
Original Assignee
Instytut Ciężkiej Syntezy Organicznej BLACHOWNIA
Polwax Spółka Akcyjna
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Instytut Ciężkiej Syntezy Organicznej BLACHOWNIA, Polwax Spółka Akcyjna filed Critical Instytut Ciężkiej Syntezy Organicznej BLACHOWNIA
Priority to PL414098A priority Critical patent/PL228523B1/en
Publication of PL414098A1 publication Critical patent/PL414098A1/en
Publication of PL228523B1 publication Critical patent/PL228523B1/en

Abstract

Sposób wytwarzania emulsji parafinowej polega na tym, że w temperaturze 80 - 99°C 100 części wagowych parafiny z ropy naftowej i/lub syntetycznej 2 - 10 części wagowych stearyny i 5 - 15 części wagowych monostearynianu gliceryny oraz 0 - 5 części wagowych etoksylowanego monostearynianu sorbitanu, 0 - 5 części wagowych monostearynianu sorbitanu, 0 - 5 części wagowych etoksylowanego monooleinianu sorbitanu i 0 - 5 części wagowych monooleinianu sorbitanu miesza się aż do uzyskania jednorodnej mieszaniny. Następnie stopniowo dozuje się roztwór zawierający 0,2 - 1,0 części wagowych wodorotlenku sodu w 60 - 250 częściach wagowych wody tak, aby temperatura w reaktorze nie obniżyła się poniżej 85 - 90°C, następnie zawartość reaktora miesza się w temperaturze 90 - 99°C jeszcze przez 10 - 60 minut, po czym wyłącza się mieszanie, całość pozostawia na kilkanaście minut w celu wstępnego odpowietrzenia, poddaje się co najmniej raz dwustopniowej homogenizacji, przepuszczając zawartość reaktora przez wysokociśnieniowy homogenizator przy ciśnieniu 5 - 60 MPa na pierwszym stopniu homogenizacji oraz przy ciśnieniu 0,1 - 10,0 MPa na drugim stopniu homogenizacji.The method of producing paraffin emulsion is that at a temperature of 80 - 99 ° C 100 parts by weight of petroleum and / or synthetic paraffin 2 - 10 parts by weight of stearin and 5 - 15 parts by weight of glycerin monostearate and 0 - 5 parts by weight of ethoxylated sorbitan monostearate 0-5 parts by weight sorbitan monostearate, 0-5 parts by weight ethoxylated sorbitan monooleate and 0-5 parts by weight sorbitan monooleate are mixed until a homogeneous mixture is obtained. Then, a solution containing 0.2 - 1.0 parts by weight of sodium hydroxide in 60 - 250 parts by weight of water is metered in gradually so that the temperature in the reactor does not drop below 85 - 90 ° C, then the contents of the reactor are stirred at 90 - 99 ° C for another 10 - 60 minutes, after which the mixing is switched off, the whole is left for several minutes for preliminary deaeration, subjected to at least once two-stage homogenization, passing the contents of the reactor through a high-pressure homogenizer at a pressure of 5 - 60 MPa at the first stage of homogenization and at a pressure of 0.1 - 10.0 MPa in the second stage of homogenization.

PL414098A 2015-09-22 2015-09-22 Method for producing paraffin emulsion PL228523B1 (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
PL414098A PL228523B1 (en) 2015-09-22 2015-09-22 Method for producing paraffin emulsion

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
PL414098A PL228523B1 (en) 2015-09-22 2015-09-22 Method for producing paraffin emulsion

Publications (2)

Publication Number Publication Date
PL414098A1 true PL414098A1 (en) 2017-03-27
PL228523B1 PL228523B1 (en) 2018-04-30

Family

ID=58360256

Family Applications (1)

Application Number Title Priority Date Filing Date
PL414098A PL228523B1 (en) 2015-09-22 2015-09-22 Method for producing paraffin emulsion

Country Status (1)

Country Link
PL (1) PL228523B1 (en)

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
PL423356A1 (en) * 2017-11-03 2019-05-06 Inst Ciezkiej Syntezy Organicznej Blachownia Method for producing paraffin-polyolefine emulsion
PL423357A1 (en) * 2017-11-03 2019-05-06 Inst Ciezkiej Syntezy Organicznej Blachownia Paraffin-polyolefin emulsion

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
PL423356A1 (en) * 2017-11-03 2019-05-06 Inst Ciezkiej Syntezy Organicznej Blachownia Method for producing paraffin-polyolefine emulsion
PL423357A1 (en) * 2017-11-03 2019-05-06 Inst Ciezkiej Syntezy Organicznej Blachownia Paraffin-polyolefin emulsion

Also Published As

Publication number Publication date
PL228523B1 (en) 2018-04-30

Similar Documents

Publication Publication Date Title
GB2505626A (en) Breaker fluids for wellbore fluids and methods of use
RU2014146228A (en) METHOD FOR PRODUCING BINDING COMPOSITION
MX2012001153A (en) EMULSION OF OIL IN FOAM WATER.
MX368069B (en) Method of making a fracturing fluid composition and utilization thereof.
MX2015010817A (en) Internal olefin sulfonate composition.
MX362992B (en) Fabric softener compositions.
PL411776A1 (en) Method for producing paraffin emulsion
PL421939A1 (en) Method for producing paraffin emulsion
RU2014128767A (en) A method of obtaining a product based on gypsum
BR112018076742A2 (en) thickener manufacturing process and use of thickeners thus produced in formulations containing high viscosity unsaturated polyester
EA201790006A1 (en) COMPOSITION OF SLIDING SOAP AND METHODS OF PRESERVING AN IMPROVED FOAMING IN WATER WITH HIGH ELECTROLYTE CONCENTRATION
MX2017010514A (en) Emulsion foam reducer for wet processing of cellulose or woodbased products or in food processing.
CN105331351B (en) A kind of degradable water base clean fracturing fluid thickening agent in oil gas field
PL439072A1 (en) Method of producing paraffin emulsion for coatings on paper packaging
MX2020006630A (en) Hardstock fat composition.
PL439071A1 (en) Method of producing paraffin-polyolefin emulsion
PL423356A1 (en) Method for producing paraffin-polyolefine emulsion
BR112016027110A8 (en) process for the production of an edible non-spillable water-in-oil emulsion
CN105441603B (en) A kind of synthetic fat liquor and preparation method thereof
CN106609131A (en) Environment-friendly synthetic based drilling fluid and preparation method thereof
MX383128B (en) METHODS OF ADDING CEMENT ADDITIVE.
GR1007663B (en) Method for the production of meat-based oil-containing products
PL408012A1 (en) Method for producing asphalt binder
RU2010127571A (en) HYDROCARBON DRILLING DRILL
PL437581A1 (en) Method for producing a paraffin-polyolefin emulsion