SU558756A1 - Способ лить выжиманием - Google Patents
Способ лить выжиманиемInfo
- Publication number
- SU558756A1 SU558756A1 SU2147393A SU2147393A SU558756A1 SU 558756 A1 SU558756 A1 SU 558756A1 SU 2147393 A SU2147393 A SU 2147393A SU 2147393 A SU2147393 A SU 2147393A SU 558756 A1 SU558756 A1 SU 558756A1
- Authority
- SU
- USSR - Soviet Union
- Prior art keywords
- metal
- cavity
- squeeze
- way
- mold
- Prior art date
Description
Изобретени;е относитс к литейному производству , в частности к получению заготовок деталей способом лить выжиманием и может ксмользоватьс дл получени отливок сложгюй кснфигур-ацк повышенной плотноети . Дл получегм крупнсгабаригных тонкостенных дстал; Л 1Г;тимсн11Ют литье выжиманием , при -.:.:-о.;„., залиьку металла произво д т в г .аск jtvyic г;аоъе.мную форму, после чего, в резу(ыате сближени частей формы металл под ймпзтс вверх, заполн ее полости и образу отливаемую деталь l . О.инако известный способ не позвол ет получать особо тонкостенные детали повышенной плотности в св зи с небольшими ско рост ми сближечи половины формы и невоз можностью создани высокого удельного да лени на мегашт. Цель изобретении. - повышение плотности и расширение номенклатуры от.чивок за счет получени особо тонкостенных деталей Это ic-стигаетсй тем, что а ппоцессе заполиени металлом полоста ие 1эл1гостью сомкнутой формы и выжимакне его нз этой полости за счет сближени половин формы к металлу прикладывают противодавление, величина которого меньше давлени , развиваемого на металл сближающимис полуформами . На фиг. 1 показана литейна форма, неполностью сомкнута в момент заливки металла в металлоприемнйк; на фиг. 2 - полностью сомкнута форма пс)сле окончани процесса лить . Форма имеет подвижную 1 и неподвижную 2 полуформы и металлопрнемник 3. Способ осуществл ют следующим образом . После неполного закрыти формы, при котором образуетс полость, превышающа по объему готовую отливку, и заливки металла в металлоприемник 3 поршнем 4 перэкрывают заливочное отверстие и вытесн ют eтaлл в упом нутую полость формы. После заполнени этой полости производ т полное смыкание формы за счет сближени полуформ 1 и 2 и вытесн ют излишек металла из нее в металлоприемник 3.