JPH0352183B2 - - Google Patents
Info
- Publication number
- JPH0352183B2 JPH0352183B2 JP57031016A JP3101682A JPH0352183B2 JP H0352183 B2 JPH0352183 B2 JP H0352183B2 JP 57031016 A JP57031016 A JP 57031016A JP 3101682 A JP3101682 A JP 3101682A JP H0352183 B2 JPH0352183 B2 JP H0352183B2
- Authority
- JP
- Japan
- Prior art keywords
- plate
- paste
- opening
- sample
- electrode plate
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Classifications
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M4/00—Electrodes
- H01M4/02—Electrodes composed of, or comprising, active material
- H01M4/14—Electrodes for lead-acid accumulators
- H01M4/16—Processes of manufacture
- H01M4/20—Processes of manufacture of pasted electrodes
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02E—REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02E60/00—Enabling technologies; Technologies with a potential or indirect contribution to GHG emissions mitigation
- Y02E60/10—Energy storage using batteries
Landscapes
- Engineering & Computer Science (AREA)
- Manufacturing & Machinery (AREA)
- Chemical & Material Sciences (AREA)
- Chemical Kinetics & Catalysis (AREA)
- Electrochemistry (AREA)
- General Chemical & Material Sciences (AREA)
- Battery Electrode And Active Subsutance (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP57031016A JPS58147959A (ja) | 1982-02-26 | 1982-02-26 | 鉛蓄電池用極板の性状判定方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP57031016A JPS58147959A (ja) | 1982-02-26 | 1982-02-26 | 鉛蓄電池用極板の性状判定方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS58147959A JPS58147959A (ja) | 1983-09-02 |
| JPH0352183B2 true JPH0352183B2 (th) | 1991-08-09 |
Family
ID=12319734
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP57031016A Granted JPS58147959A (ja) | 1982-02-26 | 1982-02-26 | 鉛蓄電池用極板の性状判定方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS58147959A (th) |
-
1982
- 1982-02-26 JP JP57031016A patent/JPS58147959A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS58147959A (ja) | 1983-09-02 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JPS6153829B2 (th) | ||
| JPH08213023A (ja) | 鉛蓄電池 | |
| JPS58147959A (ja) | 鉛蓄電池用極板の性状判定方法 | |
| JPH07211340A (ja) | 液体電解質及び電解質充填型渦巻状巻電極を備えた改良型電気化学電池 | |
| US4053686A (en) | Epoxy sealed lead battery probe | |
| US4010537A (en) | Epoxy sealed lead battery probe and method for inserting same | |
| JPS5999674A (ja) | 鉛蓄電池用格子体 | |
| JPH01304663A (ja) | 鉛蓄電池およびその製造法 | |
| JPH0782876B2 (ja) | 薄形鉛蓄電池の製造方法 | |
| JPH062206Y2 (ja) | 蓄電池 | |
| JPH0330267B2 (th) | ||
| JPS6064577U (ja) | 密閉形鉛蓄電池 | |
| JPS5842062Y2 (ja) | 絶縁塗料塗布装置 | |
| JPH0554880A (ja) | 鉛蓄電池用正極板 | |
| JPS5875765A (ja) | 鉛蓄電池用極板の製造法 | |
| JPH0446376Y2 (th) | ||
| JPS6218026Y2 (th) | ||
| JPH0541062U (ja) | 密閉形鉛蓄電池 | |
| JPH0436097Y2 (th) | ||
| JPS6179136A (ja) | 溶媒の洗浄力評価方法 | |
| JP2003217565A (ja) | 鉛蓄電池 | |
| JPS59138062A (ja) | 鉛蓄電池 | |
| JPS58209865A (ja) | 鉛蓄電池の製造法 | |
| JPH09223502A (ja) | 密閉形鉛蓄電池 | |
| JPH0530296Y2 (th) |