JPH06200084A5 - - Google Patents

Info

Publication number
JPH06200084A5
JPH06200084A5 JP4-348205A JP34820592A JPH06200084A5 JP H06200084 A5 JPH06200084 A5 JP H06200084A5 JP 34820592 A JP34820592 A JP 34820592A JP H06200084 A5 JPH06200084 A5 JP H06200084A5
Authority
JP
Japan
Prior art keywords
resin
thermoplastic resin
thermoplastic
endothermic
rubbery polymer
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP4-348205A
Other languages
English (en)
Other versions
JP3300442B2 (ja
JPH06200084A (ja
Filing date
Publication date
Application filed filed Critical
Priority to JP34820592A priority Critical patent/JP3300442B2/ja
Priority claimed from JP34820592A external-priority patent/JP3300442B2/ja
Priority to US08/171,443 priority patent/US5486543A/en
Priority to DE69326600T priority patent/DE69326600T2/de
Priority to EP93310539A priority patent/EP0605231B1/en
Publication of JPH06200084A publication Critical patent/JPH06200084A/ja
Publication of JPH06200084A5 publication Critical patent/JPH06200084A5/ja
Application granted granted Critical
Publication of JP3300442B2 publication Critical patent/JP3300442B2/ja
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Description

【手続補正書】
【提出日】平成11年12月21日(1999.12.
21)
【手続補正2】
【補正対象書類名】明細書
【補正対象項目名】0004
【補正方法】変更
【補正内容】
【0004】例えばスチレン系樹脂では、GPPS樹脂
(一般ポリスチレン)にスチレンをグラフト重合させた
ポリブタジエンやブロックSBR等のゴム質重合体を配
合したHIPS樹脂(耐衝撃性ポリスチレン)、AS樹
脂にアクリロニトリル、スチレンをグラフト重合させた
ポリブタジエンやブロックSBR等のゴム質重合体を配
合したABS樹脂、又オレフィン系樹脂では、EPM、
EPDM等のゴム質重合体を配合したPE樹脂、PP樹
脂等である。
【手続補正書】
【提出日】平成11年12月21日(1999.12.
21)
【手続補正3】
【補正対象書類名】明細書
【補正対象項目名】0006
【補正方法】変更
【補正内容】
【0006】一方後者の方法では、母材樹脂と親和性の
有る各種ゴム質重合体を要求物性に応じた配合量で、混
練押出機、等を用いて練り込み(特開61−20015
1、特告04−25975、特告01−6656、
他)、耐衝撃性の改良を行っている。
【手続補正書】
【提出日】平成11年12月21日(1999.12.
21)
【手続補正4】
【補正対象書類名】明細書
【補正対象項目名】0008
【補正方法】変更
【補正内容】
【0008】
【発明が解決しようとする課題】本願発明者は上記課題
を解決するために鋭意検討し、熱可塑性樹脂にゴム質重
合体を配合する方法について検討を行い、極めて耐衝撃
性が向上できる方法を発見し、本願発明に到達した。即
ち、本発明は、次の(1)〜(9)記載の発明に関す
る。 (1)160℃以上で分解反応を生ずる吸熱性発泡剤を
該吸熱性発泡剤の分解温度以下の温度でゴム質重合体中
へ配合した組成物を熱可塑性樹脂中へ配合した樹脂組成
物を、該吸熱性発泡剤の分解温度以上で可塑化させ成形
した耐衝撃強度を改良した熱可塑性樹脂成形物。 (2)全樹脂組成物に対するゴム質重合の配合割合が
0.5〜60wt%である(1)記載の熱可塑性樹脂成
形物。 (3)ゴム質重合体がスチレン・ブタジエンゴム、ポリ
ブタジエンゴム、ポリイソプレンゴム、EPM、EPD
M、アクリロニトル・ブタジエン共重合ゴムから選ばれ
たものである(1)記載の熱可塑性樹脂成形物。 (4)熱可塑性樹脂がポリスチレン樹脂、AS樹脂、A
BS樹脂、スチレン系樹脂、ポリエチレン樹脂、ポリプ
ロピレン樹脂から選ばれたものである(1)記載の熱可
塑性樹脂成形物。 (5)ゴム質重合体が、EPMおよび/またはEPDM
であり、熱可塑性樹脂がポリプロピレン樹脂である
(1)記載の熱可塑性樹脂成形物。 (6)ゴム質重合体が、アクリロニトル・ブタジエン共
重合ゴムであり、熱可塑性樹脂がAS樹脂、ABS樹脂
またはスチレン系樹脂である(1)記載の熱可塑性樹脂
成形物。 (7)吸熱性発泡剤がポリカルボン酸、無機炭酸化合物
から選ばれたものである(1)記載の熱可塑性樹脂成形
物。 (8)160℃以上で分解反応を生ずる吸熱性発泡剤の
ゴム質重合体に対する配合割合が0.01〜30wt%
である(1)記載の熱可塑性樹脂成形物。 (9)160℃以上で分解反応を生ずる吸熱性発泡剤を
分解温度以下の温度でゴム質重合体中へ配合した組成物
を熱可塑性樹脂中へ配合した樹脂組成物を、該吸熱性発
泡剤の分解温度以上で可塑化させ成形することを特徴と
する熱可塑性樹脂成形物の耐衝撃強度の改良方法。
【手続補正書】
【提出日】平成11年12月21日(1999.12.
21)
【手続補正5】
【補正対象書類名】明細書
【補正対象項目名】0012
【補正方法】変更
【補正内容】
【0012】ゴム質重合体に対する吸熱性発泡剤の使用
量は、吸熱発泡剤の種類によっても異なるが、一般には
ゴム質重合体に対して0.01〜30wt%,好ましくは
0.05〜5.0wt% 、更に好ましくは0.2〜3wt%
の範囲であり、この範囲で適宜選択することができる。
特に、吸熱性発泡剤としてカルボン酸と無機炭酸化合
物を用いた場合はゴム質重合体に対して0.2から〜
4.0wt% の範囲が好ましい。この吸熱性発泡剤はマス
ターバッチとして高濃度の物を使用することができるが
この場合の使用量は樹脂に添加されるゴム質重合体全量
に対しての割合で決定される。 これらゴム質重合体中
へ上記吸熱性発泡剤を配合する場合、その後発泡剤の分
解温度以下で配合することが必要である。ゴム質重合体
中への吸熱性発泡剤の配合方法としては、その発泡剤の
分解温度以下で一軸或いは二軸混練押出機を用いて練り
込むか、バンバリーミキサー、コ・ニーダー等を用いて
練り込む方法が一般的ある。この際、吸熱性発泡剤は直
接、或いは予め他の熱可塑性成分によって高濃度化した
マスターバッチとしたものを用いても良く、更に同時に
ゴム質重合体へ可塑剤、分散剤等各種添加剤を練り込む
ことも出来る。
【手続補正書】
【提出日】平成11年12月21日(1999.12.
21)
【手続補正6】
【補正対象書類名】明細書
【補正対象項目名】0016
【補正方法】変更
【補正内容】
【0016】熱可塑性樹脂とゴム質重合体の配合割合は
通常熱可塑性樹脂にゴム質重合体を混合して耐衝撃性を
改良する通常の方法で添加される公知の割合が好まし
く、一般にはゴム質重合体を熱可塑性樹脂に対して0.
5〜60wt% 、好ましくは0.8〜30wt% 、更に好ま
しくは1.0〜20wt% 添加するのが好ましい。これよ
りゴム質重合体が多くなると剛性が低下し、また本願発
明の効果である吸熱発泡剤の添加効果を奏しないし、ま
たこれより少ないと耐衝撃性の向上効果をしめさない。
上記の範囲で目標とする物性になるように組成を自由に
選択することができる。例えば、本願の発明では同じゴ
ム質重合体の使用量で高い耐衝撃性が得られるので、同
じ耐衝撃性の成形物を得るためにはゴム質重合体の使用
量を減少できるので、より剛性と耐衝撃性のバランスの
良好な成形物が得られる。
【手続補正書】
【提出日】平成11年12月21日(1999.12.
21)
【手続補正7】
【補正対象書類名】明細書
【補正対象項目名】0024
【補正方法】変更
【補正内容】
【0024】実施例−1 樹脂組成物B・1を成形温度210℃、230℃で成形
した実験結果を表−1−1に示す(以降、表中における
成形物物性の単位は、それぞれ、アイゾット衝撃強さ
(Kg・cm)、曲げ弾性率(Kgf/cm)、加熱変
形温度(℃)、光沢(度)である。)。

Claims (9)

    【手続補正書】 【提出日】平成11年12月21日(1999.12.21) 【手続補正1】 【補正対象書類名】明細書 【補正対象項目名】特許請求の範囲 【補正方法】変更 【補正内容】 【特許請求の範囲】
  1. 【請求項1】160℃以上で分解反応を生ずる吸熱性発
    泡剤を該吸熱性発泡剤の分解温度以下の温度でゴム質重
    合体中へ配合した組成物を熱可塑性樹脂中へ配合した樹
    脂組成物を、該吸熱性発泡剤の分解温度以上で可塑化さ
    せ成形した耐衝撃強度を改良した熱可塑性樹脂成形物。
  2. 【請求項2】全樹脂組成物に対するゴム質重合の配合割
    合が0.5〜60wt%である請求項1記載の熱可塑性
    樹脂成形物。
  3. 【請求項3】ゴム質重合体がスチレン・ブタジエンゴ
    ム、ポリブタジエンゴム、ポリイソプレンゴム、EP
    M、EPDM、アクリロニトル・ブタジエン共重合ゴム
    から選ばれたものである請求項1記載の熱可塑性樹脂成
    形物。
  4. 【請求項4】熱可塑性樹脂がポリスチレン樹脂、AS樹
    脂、ABS樹脂、スチレン系樹脂、ポリエチレン樹脂、
    ポリプロピレン樹脂から選ばれたものである請求項1記
    載の熱可塑性樹脂成形物。
  5. 【請求項5】ゴム質重合体が、EPMおよび/またはE
    PDMであり、熱可塑性樹脂がポリプロピレン樹脂であ
    る請求項1記載の熱可塑性樹脂成形物。
  6. 【請求項6】ゴム質重合体が、アクリロニトル・ブタジ
    エン共重合ゴムであり、熱可塑性樹脂がAS樹脂、AB
    S樹脂またはスチレン系樹脂である請求項1記載の熱可
    塑性樹脂成形物。
  7. 【請求項7】吸熱性発泡剤がポリカルボン酸、無機炭酸
    化合物から選ばれたものである請求項1記載の熱可塑性
    樹脂成形物。
  8. 【請求項8】160℃以上で分解反応を生ずる吸熱性発
    泡剤のゴム質重合体に対する配合割合が0.01〜30
    wt%である請求項1記載の熱可塑性樹脂成形物。
  9. 【請求項9】160℃以上で分解反応を生ずる吸熱性発
    泡剤を分解温度以下の温度でゴム質重合体中へ配合した
    組成物を熱可塑性樹脂中へ配合した樹脂組成物を、該吸
    熱性発泡剤の分解温度以上で可塑化させ成形することを
    特徴とする熱可塑性樹脂成形物の耐衝撃強度の改良方
    法。
JP34820592A 1992-12-28 1992-12-28 熱可塑性樹脂成形物の耐衝撃強度の改良方法及びそのための組成物 Expired - Lifetime JP3300442B2 (ja)