JPS5584201A - Surface cracking suppressing method of slab at hot rolling - Google Patents
Surface cracking suppressing method of slab at hot rollingInfo
- Publication number
- JPS5584201A JPS5584201A JP15666778A JP15666778A JPS5584201A JP S5584201 A JPS5584201 A JP S5584201A JP 15666778 A JP15666778 A JP 15666778A JP 15666778 A JP15666778 A JP 15666778A JP S5584201 A JPS5584201 A JP S5584201A
- Authority
- JP
- Japan
- Prior art keywords
- slab
- rolling
- surface cracking
- hot rolling
- suppressing method
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
PURPOSE:To effectively suppress surface cracking by rolling a slab after subjecting the same to holding for the specified time in the specific temperature region of cooling process in succession to melting and solidifying in direct feed rolling, etc. of the slab. CONSTITUTION:In direct feed rolling or hot charge rolling of a slab, the slab is subjected to holding for 10 minutes or more in the temperature region of 1,150- 950 deg.C in the cooling process in succession to melting and solidifying, whereby harmful deposits are made harmless. Hot rolling is performed after this. Thereby, the slab surface cracking at the hot rolling may be effectively suppressed.
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP53156667A JPS5852442B2 (en) | 1978-12-19 | 1978-12-19 | Method for suppressing surface cracking of steel billet during hot rolling |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP53156667A JPS5852442B2 (en) | 1978-12-19 | 1978-12-19 | Method for suppressing surface cracking of steel billet during hot rolling |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS5584201A true JPS5584201A (en) | 1980-06-25 |
| JPS5852442B2 JPS5852442B2 (en) | 1983-11-22 |
Family
ID=15632662
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP53156667A Expired JPS5852442B2 (en) | 1978-12-19 | 1978-12-19 | Method for suppressing surface cracking of steel billet during hot rolling |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS5852442B2 (en) |
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS62212001A (en) * | 1986-03-13 | 1987-09-18 | Sumitomo Metal Ind Ltd | Hot rolling method for preventing surface cracking of ingot |
Families Citing this family (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS60218529A (en) * | 1984-04-13 | 1985-11-01 | Mitsubishi Electric Corp | Combustion state detection device |
Citations (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS52105520A (en) * | 1976-03-02 | 1977-09-05 | Nippon Steel Corp | Continuous casting and continuous hot rolling of aluminium-killed stee l |
| JPS52108319A (en) * | 1976-03-10 | 1977-09-10 | Nippon Steel Corp | Production of high strength steel sheet |
| JPS52131919A (en) * | 1976-04-28 | 1977-11-05 | Nippon Steel Corp | Production of a1-s# killed steel plate by direct fot rolling of continuous cast slab |
| JPS5333919A (en) * | 1976-09-10 | 1978-03-30 | Nippon Steel Corp | Production of cold rolled aluminum killed steel sheet with excellent deep drawability |
-
1978
- 1978-12-19 JP JP53156667A patent/JPS5852442B2/en not_active Expired
Patent Citations (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS52105520A (en) * | 1976-03-02 | 1977-09-05 | Nippon Steel Corp | Continuous casting and continuous hot rolling of aluminium-killed stee l |
| JPS52108319A (en) * | 1976-03-10 | 1977-09-10 | Nippon Steel Corp | Production of high strength steel sheet |
| JPS52131919A (en) * | 1976-04-28 | 1977-11-05 | Nippon Steel Corp | Production of a1-s# killed steel plate by direct fot rolling of continuous cast slab |
| JPS5333919A (en) * | 1976-09-10 | 1978-03-30 | Nippon Steel Corp | Production of cold rolled aluminum killed steel sheet with excellent deep drawability |
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS62212001A (en) * | 1986-03-13 | 1987-09-18 | Sumitomo Metal Ind Ltd | Hot rolling method for preventing surface cracking of ingot |
Also Published As
| Publication number | Publication date |
|---|---|
| JPS5852442B2 (en) | 1983-11-22 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| DE2967018D1 (en) | Method of treating the surfaces of high carbon steel bodies | |
| PH16201A (en) | Method and apparatus for hot forming metals prone to crack during forming | |
| JPS5584201A (en) | Surface cracking suppressing method of slab at hot rolling | |
| JPS5584203A (en) | Surface cracking suppressing method of slab at hot rolling | |
| JPS5584202A (en) | Surface cracking suppressing method of slab in hot rolling | |
| JPS5638499A (en) | Preparation of ba (bright annealing finish) product of chrome stainless steel with retarded generation of whitening on product surface | |
| JPS51115770A (en) | Annealing method after ion injection | |
| JPS54106061A (en) | Blooming method for killed steel | |
| JPS53112248A (en) | Method and facilities for hot direct rolling of steel material | |
| JPS5362713A (en) | Method and apparatus for cooling steel belt | |
| JPS5315206A (en) | Turning over apparatus for steel pieces | |
| JPS5588903A (en) | Manufacture of hot coil of continuously casting slab for stainless steel by direct feed rolling | |
| JPS5575944A (en) | Glass surface treating method | |
| JPS5438661A (en) | Method of treating refuse | |
| JPS53138961A (en) | Carrying and treating apparatus of casting slab for continuous casting equipment | |
| JPS542219A (en) | Heat treating method for alloy 800 seamless pipe formed from centrifugal cast pipe as rough pipe | |
| JPS53134771A (en) | Method and apparatus for insolublization treatment of sludge | |
| JPS51137154A (en) | Heating method for processing steel bars etc. | |
| JPS5536018A (en) | Flash welding method | |
| JPS5395131A (en) | Removing method for scale of steel | |
| JPS5597459A (en) | Surface treatment | |
| JPS5387164A (en) | Heat traetment method of compound crystal | |
| JPS5242367A (en) | Method of preventing occurence of crystal defects of silicon wafers | |
| JPS5510307A (en) | Removing method of cross gate of casting | |
| JPS53109830A (en) | Welding method for prevention of reheating crack |