JPS62290823A - 密着性に優れた表面被膜をそなえる超低鉄損一方向性けい素鋼板の製造方法 - Google Patents
密着性に優れた表面被膜をそなえる超低鉄損一方向性けい素鋼板の製造方法Info
- Publication number
- JPS62290823A JPS62290823A JP13108186A JP13108186A JPS62290823A JP S62290823 A JPS62290823 A JP S62290823A JP 13108186 A JP13108186 A JP 13108186A JP 13108186 A JP13108186 A JP 13108186A JP S62290823 A JPS62290823 A JP S62290823A
- Authority
- JP
- Japan
- Prior art keywords
- steel sheet
- silicon steel
- annealing
- ion plating
- mirror
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Chemical Treatment Of Metals (AREA)
- Physical Vapour Deposition (AREA)
- Manufacturing Of Steel Electrode Plates (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP13108186A JPS62290823A (ja) | 1986-06-07 | 1986-06-07 | 密着性に優れた表面被膜をそなえる超低鉄損一方向性けい素鋼板の製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP13108186A JPS62290823A (ja) | 1986-06-07 | 1986-06-07 | 密着性に優れた表面被膜をそなえる超低鉄損一方向性けい素鋼板の製造方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS62290823A true JPS62290823A (ja) | 1987-12-17 |
| JPH0327632B2 JPH0327632B2 (mo) | 1991-04-16 |
Family
ID=15049544
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP13108186A Granted JPS62290823A (ja) | 1986-06-07 | 1986-06-07 | 密着性に優れた表面被膜をそなえる超低鉄損一方向性けい素鋼板の製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS62290823A (mo) |
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2012035302A (ja) * | 2010-08-06 | 2012-02-23 | Jfe Steel Corp | 電子ビーム照射装置 |
-
1986
- 1986-06-07 JP JP13108186A patent/JPS62290823A/ja active Granted
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2012035302A (ja) * | 2010-08-06 | 2012-02-23 | Jfe Steel Corp | 電子ビーム照射装置 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0327632B2 (mo) | 1991-04-16 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| WO1986002950A1 (fr) | Procede de fabrication de plaques d'acier electromagnetique unidirectionnel a faible perte de fer | |
| JPH0672266B2 (ja) | 超低鉄損一方向性珪素鋼板の製造方法 | |
| JP2653638B2 (ja) | 鉄損の低い方向性電磁鋼板の製造方法 | |
| JPS61235514A (ja) | 熱安定性、超低鉄損一方向性珪素鋼板の製造方法 | |
| JPS621821A (ja) | ひずみ取り焼鈍を施しても特性劣化のない超低鉄損一方向性珪素鋼板の製造方法 | |
| JPS61201732A (ja) | 熱安定性、超低鉄損一方向性珪素鋼板の製造方法 | |
| JP3148092B2 (ja) | 鉄損の低い鏡面方向性電磁鋼板の製造方法 | |
| JPH0327632B2 (mo) | ||
| JP3148093B2 (ja) | 鉄損の低い鏡面方向性電磁鋼板の製造方法 | |
| JPS63227719A (ja) | 超低鉄損一方向性珪素鋼板の製造方法 | |
| JPS621822A (ja) | 熱安定性、超低鉄損一方向性珪素鋼板の製造方法 | |
| JPS62192581A (ja) | 超低鉄損一方向性けい素鋼板の製造方法 | |
| JPH01159322A (ja) | 超低鉄損一方向性珪素鋼板の製造方法 | |
| JPH0699823B2 (ja) | 超低鉄損一方向性珪素鋼板の製造方法 | |
| JPS6230302A (ja) | 超低鉄損一方向性けい素鋼板の製造方法 | |
| JPS6318087A (ja) | 低鉄損一方向性けい素鋼板の製造方法 | |
| JPH0335377B2 (mo) | ||
| JPS6229107A (ja) | 超低鉄損一方向性珪素鋼板の製造方法 | |
| JPH0327633B2 (mo) | ||
| JPH01198430A (ja) | 極めて鉄損が優れ、被膜密着性の優れた方向性電磁鋼板の製造方法 | |
| JPS61246321A (ja) | 超低鉄損一方向性珪素鋼板の製造方法 | |
| JPS6263408A (ja) | 超低鉄損一方向性けい素鋼板の製造方法 | |
| JPS6324017A (ja) | 低鉄損一方向性けい素鋼板の製造方法 | |
| JPS6222409A (ja) | 超低鉄損一方向性珪素鋼板の製造方法 | |
| JPS6324099A (ja) | 低鉄損一方向性けい素鋼板の製造方法 |