PL384343A3 - Sposób nawęglania kąpieli metalowej - Google Patents

Sposób nawęglania kąpieli metalowej

Info

Publication number
PL384343A3
PL384343A3 PL384343A PL38434308A PL384343A3 PL 384343 A3 PL384343 A3 PL 384343A3 PL 384343 A PL384343 A PL 384343A PL 38434308 A PL38434308 A PL 38434308A PL 384343 A3 PL384343 A3 PL 384343A3
Authority
PL
Poland
Prior art keywords
metal bath
carburizing
intensification
carbureting
gaseous oxygen
Prior art date
Application number
PL384343A
Other languages
English (en)
Other versions
PL211387B1 (pl
Inventor
Lech Bulkowski
Bogdan Zdonek
Kazimierz Ochab
Marian Rachwalski
Original Assignee
Instytut Metalurgii Żelaza im. Stanisława Staszica
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Instytut Metalurgii Żelaza im. Stanisława Staszica filed Critical Instytut Metalurgii Żelaza im. Stanisława Staszica
Priority to PL384343A priority Critical patent/PL211387B1/pl
Publication of PL384343A3 publication Critical patent/PL384343A3/pl
Publication of PL211387B1 publication Critical patent/PL211387B1/pl

Abstract

Sposób nawęglania kąpieli metalowej, polegający na nawęglaniu kąpieli metalowej materiałem węglistym i topieniu wsadu z intensyfikacją tlenem gazowym według patentu nr 194453 (zgłoszenia nr P.349691), realizuje się tak, że jako nawęglacz stosuje się niepełnowartościowy półprodukt z produkcji opon w postaci bloku zbitej masy kompozytu gumowo-stalowego, który umieszcza się w koszu wsadowym na warstwę złomu lekkiego, po czym kosz napełnia się złomem i ładuje do pieca z pozostawionym w nim jeziorkiem ciekłego metalu z poprzedniego wytopu, korzystnie o temperaturze 1450°C do 1650°C, a następnie całość poddaje się procesowi topienia, korzystnie z intensyfikacją tlenem gazowym.
PL384343A 2008-01-29 2008-01-29 Sposób nawęglania kąpieli metalowej PL211387B1 (pl)

Priority Applications (1)

Application Number Priority Date Filing Date Title
PL384343A PL211387B1 (pl) 2008-01-29 2008-01-29 Sposób nawęglania kąpieli metalowej

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
PL384343A PL211387B1 (pl) 2008-01-29 2008-01-29 Sposób nawęglania kąpieli metalowej

Publications (2)

Publication Number Publication Date
PL384343A3 true PL384343A3 (pl) 2009-08-03
PL211387B1 PL211387B1 (pl) 2012-05-31

Family

ID=42987013

Family Applications (1)

Application Number Title Priority Date Filing Date
PL384343A PL211387B1 (pl) 2008-01-29 2008-01-29 Sposób nawęglania kąpieli metalowej

Country Status (1)

Country Link
PL (1) PL211387B1 (pl)

Also Published As

Publication number Publication date
PL211387B1 (pl) 2012-05-31

Similar Documents

Publication Publication Date Title
PL2152487T3 (pl) Włókno węglowe do recyklingu
EP2261193A4 (en) ZIRCONIUM OXIDE / CARBON CONTAINING REFRACTORY MATERIAL AND METHOD OF MANUFACTURING THEREOF
EA201491429A1 (ru) Способ производства минеральной ваты
EA201891065A1 (ru) Способ и устройство для предварительного нагрева и плавки агломерата марганцевой руды
RU2013144611A (ru) Способ прямого плавления сырья с высоким содержанием серы
BR112016014464A2 (pt) método para produção de aço em uma fornalha de arco elétrico e fornalha de arco elétrico
RU2013116982A (ru) Способ прямой плавки
NZ735530A (en) Method and apparatus for treating iron-containing raw material using bath smelting furnace
UA116350C2 (uk) Спосіб і установка для збільшення теплотворної здатності потоку вуглецевмісного матеріалу
PL384343A3 (pl) Sposób nawęglania kąpieli metalowej
WO2010050676A3 (ko) 경금속의 진공용해장치 및 이를 이용한 진공용해방법
IN2014CN04231A (pl)
IN2014CN04192A (pl)
UA92686C2 (uk) Спосіб і пристрій для виробництва мінеральних волокон
EA201390127A1 (ru) Способ легирования полупроводникового материала
RU2009103499A (ru) Способ введения упрочняющих частиц в алюминиевые сплавы
RU2009134352A (ru) Способ получения слоистых слитков импульсно-электрошлаковым переплавом
TWI412600B (zh) Method of Reducing Phosphorus Content
RU2015121452A (ru) Способ переработки низкоавтогенного сырья в печах взвешенной плавки
UA40646U (ru) Способ кислородно-конверторной выплавки стали
EA200601537A1 (ru) Комбинированный способ предварительной обработки сырья, загружаемого в печь для прямого восстановления
RU2007148143A (ru) Способ выплавки стали
RU2008136250A (ru) Способ получения металлов и сплавов путем восстановительной плавки и устройство для его осуществления
Abraham et al. EAF energy and material balance modeling
AR133811A1 (es) Proceso para producir acero limpio y producto de acero limpio con bajo contenido de nitrógeno