JPH0411607A - 塩化ビニル系重合体の製造方法 - Google Patents
塩化ビニル系重合体の製造方法Info
- Publication number
- JPH0411607A JPH0411607A JP11545490A JP11545490A JPH0411607A JP H0411607 A JPH0411607 A JP H0411607A JP 11545490 A JP11545490 A JP 11545490A JP 11545490 A JP11545490 A JP 11545490A JP H0411607 A JPH0411607 A JP H0411607A
- Authority
- JP
- Japan
- Prior art keywords
- polymerization
- vinyl chloride
- oil
- added
- soluble
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Links
Landscapes
- Polymerisation Methods In General (AREA)
- Polymerization Catalysts (AREA)
Priority Applications (3)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP11545490A JPH0411607A (ja) | 1990-05-01 | 1990-05-01 | 塩化ビニル系重合体の製造方法 |
| PT9753391A PT97533B (pt) | 1990-05-01 | 1991-04-30 | Processo aperfeicoado para a polimerizacao em suspensao de cloreto de vinilo |
| CA 2041540 CA2041540A1 (en) | 1990-05-01 | 1991-04-30 | Suspension polymerization of vinyl chloride |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP11545490A JPH0411607A (ja) | 1990-05-01 | 1990-05-01 | 塩化ビニル系重合体の製造方法 |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| JPH0411607A true JPH0411607A (ja) | 1992-01-16 |
Family
ID=14662954
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP11545490A Pending JPH0411607A (ja) | 1990-05-01 | 1990-05-01 | 塩化ビニル系重合体の製造方法 |
Country Status (3)
| Country | Link |
|---|---|
| JP (1) | JPH0411607A (pt) |
| CA (1) | CA2041540A1 (pt) |
| PT (1) | PT97533B (pt) |
-
1990
- 1990-05-01 JP JP11545490A patent/JPH0411607A/ja active Pending
-
1991
- 1991-04-30 CA CA 2041540 patent/CA2041540A1/en not_active Abandoned
- 1991-04-30 PT PT9753391A patent/PT97533B/pt not_active IP Right Cessation
Also Published As
| Publication number | Publication date |
|---|---|
| PT97533B (pt) | 1998-08-31 |
| PT97533A (pt) | 1992-01-31 |
| CA2041540A1 (en) | 1991-11-02 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JP2583453B2 (ja) | 可塑剤吸収性の改良された塩化ビニル系重合体の製造方法 | |
| JP4024482B2 (ja) | 塩化ビニル系重合体の製造方法 | |
| JPH0118082B2 (pt) | ||
| JP3169673B2 (ja) | 塩化ビニル系重合体の製造方法 | |
| JP2986276B2 (ja) | 塩化ビニル系重合体の製造方法 | |
| JPH0411607A (ja) | 塩化ビニル系重合体の製造方法 | |
| JPH02305804A (ja) | 塩化ビニル系重合体の製造方法 | |
| JP2823681B2 (ja) | 塩化ビニル系重合体の製造方法 | |
| JP2962615B2 (ja) | 塩化ビニル系重合体の製造方法 | |
| JP3210504B2 (ja) | 塩化ビニル系重合体の製造方法 | |
| JPH0411606A (ja) | 塩化ビニル系重合体の製造方法 | |
| JPH05279405A (ja) | 塩化ビニル系重合体の製造方法 | |
| JP3115919B2 (ja) | 塩化ビニル系重合体の製造方法 | |
| JP4098482B2 (ja) | 塩化ビニル系重合体の製造方法 | |
| JPH0565313A (ja) | 塩化ビニル系重合体の製造方法 | |
| JP3414026B2 (ja) | 塩化ビニル系重合体の製造方法 | |
| JPH0778083B2 (ja) | 塩化ビニル系懸濁重合方法における懸濁安定剤の仕込み方法 | |
| JP3284723B2 (ja) | 塩化ビニル系重合体の製造方法 | |
| JPH04325506A (ja) | 塩化ビニル系重合体の製造方法 | |
| JPH0539309A (ja) | 塩化ビニル系重合体の製造方法 | |
| JPH05222105A (ja) | 塩化ビニル系重合体の製造方法 | |
| JP3437018B2 (ja) | 塩化ビニル系重合体の製造方法 | |
| JP3340275B2 (ja) | 塩化ビニル系重合体の製造方法 | |
| JPH09278806A (ja) | 塩化ビニル系単量体の懸濁重合方法 | |
| JPH03269005A (ja) | 塩化ビニル系単量体の懸濁重合方法 |