JPH1040905A - 疎水性極板および疎水性成形物の製造方法 - Google Patents
疎水性極板および疎水性成形物の製造方法Info
- Publication number
- JPH1040905A JPH1040905A JP9107971A JP10797197A JPH1040905A JP H1040905 A JPH1040905 A JP H1040905A JP 9107971 A JP9107971 A JP 9107971A JP 10797197 A JP10797197 A JP 10797197A JP H1040905 A JPH1040905 A JP H1040905A
- Authority
- JP
- Japan
- Prior art keywords
- hydrophobic
- electrode plate
- producing
- battery
- dispersion
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Links
Classifications
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M10/00—Secondary cells; Manufacture thereof
- H01M10/42—Methods or arrangements for servicing or maintenance of secondary cells or secondary half-cells
- H01M10/52—Removing gases inside the secondary cell, e.g. by absorption
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M4/00—Electrodes
- H01M4/02—Electrodes composed of, or comprising, active material
- H01M4/24—Electrodes for alkaline accumulators
- H01M4/26—Processes of manufacture
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M4/00—Electrodes
- H01M4/02—Electrodes composed of, or comprising, active material
- H01M4/24—Electrodes for alkaline accumulators
- H01M4/32—Nickel oxide or hydroxide electrodes
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M10/00—Secondary cells; Manufacture thereof
- H01M10/34—Gastight accumulators
- H01M10/345—Gastight metal hydride accumulators
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02E—REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02E60/00—Enabling technologies; Technologies with a potential or indirect contribution to GHG emissions mitigation
- Y02E60/10—Energy storage using batteries
Landscapes
- Chemical & Material Sciences (AREA)
- Chemical Kinetics & Catalysis (AREA)
- Electrochemistry (AREA)
- General Chemical & Material Sciences (AREA)
- Manufacturing & Machinery (AREA)
- Engineering & Computer Science (AREA)
- Battery Electrode And Active Subsutance (AREA)
- Cell Separators (AREA)
- Application Of Or Painting With Fluid Materials (AREA)
- Coating Of Shaped Articles Made Of Macromolecular Substances (AREA)
- Separation Using Semi-Permeable Membranes (AREA)
- Solid-Sorbent Or Filter-Aiding Compositions (AREA)
- Fuel Cell (AREA)
Applications Claiming Priority (2)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| KR1019960019135A KR0172229B1 (ko) | 1996-05-31 | 1996-05-31 | 소수성 극판의 제조 방법 |
| KR1996-19135 | 1996-05-31 |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| JPH1040905A true JPH1040905A (ja) | 1998-02-13 |
Family
ID=19460386
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP9107971A Pending JPH1040905A (ja) | 1996-05-31 | 1997-04-25 | 疎水性極板および疎水性成形物の製造方法 |
Country Status (11)
| Country | Link |
|---|---|
| JP (1) | JPH1040905A (ko) |
| KR (1) | KR0172229B1 (ko) |
| CN (1) | CN1170247A (ko) |
| DE (1) | DE19716704A1 (ko) |
| ES (1) | ES2125832B1 (ko) |
| FR (1) | FR2749195A1 (ko) |
| GB (1) | GB2313561A (ko) |
| IT (1) | IT1291648B1 (ko) |
| NL (1) | NL1006184C2 (ko) |
| SE (1) | SE9701907L (ko) |
| SG (1) | SG71706A1 (ko) |
Families Citing this family (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| CN1085896C (zh) * | 1997-12-19 | 2002-05-29 | 王纪三 | 充电电池的电极和电极制造方法及其设备 |
| US9023556B2 (en) | 2006-03-17 | 2015-05-05 | GM Global Technology Operations LLC | Method of preparing gas diffusion media for a fuel cell |
| JP5975307B2 (ja) * | 2012-11-28 | 2016-08-23 | パナソニックIpマネジメント株式会社 | ニッケル水素蓄電池および組電池 |
| CN117960702A (zh) * | 2024-02-02 | 2024-05-03 | 深圳市资福医疗技术有限公司 | 软包电池及其清洗方法、内窥镜、装置、设备及存储介质 |
Family Cites Families (15)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5214749B2 (ko) * | 1972-12-22 | 1977-04-23 | ||
| JPS5112643A (en) * | 1974-07-19 | 1976-01-31 | Matsushita Electric Industrial Co Ltd | Denchokyokubanno seizoho |
| JPS5372139A (en) * | 1976-12-09 | 1978-06-27 | Matsushita Electric Industrial Co Ltd | Method of manufacturing positive electrode plate for alkaline storage battery |
| EP0077326A4 (en) * | 1981-04-28 | 1983-07-26 | Diamond Shamrock Corp | Method of depositing cation exchange membrane on a foraminous cathode. |
| FR2513906A1 (fr) * | 1981-10-06 | 1983-04-08 | Morin Joel | Procede et composition pour la mise en place d'un revetement anti-adherent et auto-lubrifiant |
| US4503099A (en) * | 1983-06-15 | 1985-03-05 | Borg-Warner Corporation | Heat transfer surfaces having scale resistant polymer coatings thereon |
| JPH01143141A (ja) * | 1987-11-27 | 1989-06-05 | Shin Kobe Electric Mach Co Ltd | 電極の製造方法 |
| US5034289A (en) * | 1989-02-23 | 1991-07-23 | Matsushita Electric Industrial Co., Ltd. | Alkaline storage battery and method of producing negative electrode thereof |
| JPH02227966A (ja) * | 1989-02-28 | 1990-09-11 | Matsushita Electric Ind Co Ltd | 密閉形アルカリ蓄電池とその負極の製造法 |
| JP2918560B2 (ja) * | 1989-03-09 | 1999-07-12 | 古河電池株式会社 | 水素吸蔵電極の製造法 |
| US5242765A (en) * | 1992-06-23 | 1993-09-07 | Luz Electric Fuel Israel Limited | Gas diffusion electrodes |
| JPH0660871A (ja) * | 1992-08-07 | 1994-03-04 | Nippon Oil Co Ltd | アルカリ蓄電池用亜鉛負極及びその製造方法 |
| JPH0660876A (ja) * | 1992-08-12 | 1994-03-04 | Nippon Oil Co Ltd | アルカリ蓄電池及びその製造方法 |
| DE4326944A1 (de) * | 1993-08-11 | 1995-02-16 | Varta Batterie | Negative Elektrode für gasdichte alkalische Akkumulatoren, die eine Ruß enthaltende Gasverzehrschicht besitzt |
| JPH07240200A (ja) * | 1994-02-28 | 1995-09-12 | Fuji Photo Film Co Ltd | 非水二次電池 |
-
1996
- 1996-05-31 KR KR1019960019135A patent/KR0172229B1/ko not_active Expired - Fee Related
-
1997
- 1997-04-18 ES ES009700839A patent/ES2125832B1/es not_active Expired - Lifetime
- 1997-04-21 DE DE19716704A patent/DE19716704A1/de not_active Withdrawn
- 1997-04-22 SG SG1997001274A patent/SG71706A1/en unknown
- 1997-04-22 GB GB9708085A patent/GB2313561A/en not_active Withdrawn
- 1997-04-24 IT IT97MI000955A patent/IT1291648B1/it active IP Right Grant
- 1997-04-25 JP JP9107971A patent/JPH1040905A/ja active Pending
- 1997-05-15 CN CN97111404A patent/CN1170247A/zh active Pending
- 1997-05-20 FR FR9706124A patent/FR2749195A1/fr not_active Withdrawn
- 1997-05-22 SE SE9701907A patent/SE9701907L/xx not_active Application Discontinuation
- 1997-05-30 NL NL1006184A patent/NL1006184C2/nl not_active IP Right Cessation
Also Published As
| Publication number | Publication date |
|---|---|
| GB9708085D0 (en) | 1997-06-11 |
| SE9701907L (sv) | 1997-12-01 |
| KR970077787A (ko) | 1997-12-12 |
| NL1006184A1 (nl) | 1997-12-03 |
| GB2313561A (en) | 1997-12-03 |
| DE19716704A1 (de) | 1997-12-04 |
| ES2125832B1 (es) | 1999-11-16 |
| SG71706A1 (en) | 2000-04-18 |
| NL1006184C2 (nl) | 1999-06-08 |
| KR0172229B1 (ko) | 1999-03-30 |
| IT1291648B1 (it) | 1999-01-19 |
| SE9701907D0 (sv) | 1997-05-22 |
| ES2125832A1 (es) | 1999-03-01 |
| FR2749195A1 (fr) | 1997-12-05 |
| ITMI970955A0 (ko) | 1997-04-24 |
| CN1170247A (zh) | 1998-01-14 |
| ITMI970955A1 (it) | 1998-10-24 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JP2003508885A (ja) | 水に対する濡れ性の向上した多孔質炭素体 | |
| JPH1040905A (ja) | 疎水性極板および疎水性成形物の製造方法 | |
| US6017635A (en) | Hydrophobic composition and a method of preparing a hydrophobic plate | |
| US5514497A (en) | Paste nickel electrode plate and a storage battery including an electroconductive material | |
| JP2012049016A (ja) | 電極の製造方法および電極前駆体の処理方法 | |
| CN1739210A (zh) | 密闭型镍氢蓄电池及其制造方法 | |
| EP0602768A2 (en) | Hydrogen-absorbing alloy electrode and manufacturing method therefor | |
| JP2006059732A (ja) | 非水電解液電池 | |
| CN1790786A (zh) | 碱性电池及其生产方法 | |
| JP2020170652A (ja) | 亜鉛電池用負極の製造方法、及び亜鉛電池用負極 | |
| JPH09204919A (ja) | アルカリ電池用電極基板およびその製造方法 | |
| JP3749001B2 (ja) | 焼結式カドミウム負極およびその製造方法 | |
| JP2686136B2 (ja) | アルカリ蓄電池用カドミウム負極 | |
| JP2000164222A (ja) | Liイオン電池の陰極集電部材用銅材、およびLiイオン電池用陰極集電部材の製造方法 | |
| JPH0799690B2 (ja) | 水素吸蔵電極の製造方法 | |
| KR19980059087A (ko) | 니켈 계열 전지용 음극 및 이의 제조 방법 | |
| JP3448886B2 (ja) | アルカリ蓄電池用カドミウム負極板の製造方法 | |
| MXPA97006616A (en) | A hydrophobic composition and a method for preparing a hydrofob plate | |
| KR19980059072A (ko) | 소수성 극판의 제조 방법 | |
| KR980010577A (ko) | 니켈 계열 전지의 음극용 조성물 및 이의 제조 방법 | |
| KR980012677A (ko) | 니켈 계열 전지의 음극용 조성물 및 이의 제조 방법 | |
| JP2006221834A (ja) | 有機電解液電池用正極および有機電解液電池の製造方法 | |
| JPS61190861A (ja) | アルカリ蓄電池用カドミウム陰極 | |
| CN119297215A (zh) | 应用于碱性镍锌电池的正电极及其制备方法 | |
| JPH08203515A (ja) | ニッケル電極の製造方法 |