JPS623092A - BaPbO3系酸化物超伝導体単結晶の溶液引上げ法による製造方法 - Google Patents
BaPbO3系酸化物超伝導体単結晶の溶液引上げ法による製造方法Info
- Publication number
- JPS623092A JPS623092A JP60143189A JP14318985A JPS623092A JP S623092 A JPS623092 A JP S623092A JP 60143189 A JP60143189 A JP 60143189A JP 14318985 A JP14318985 A JP 14318985A JP S623092 A JPS623092 A JP S623092A
- Authority
- JP
- Japan
- Prior art keywords
- single crystal
- melt
- mixed
- crystal
- microcrystal
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Crystals, And After-Treatments Of Crystals (AREA)
- Liquid Deposition Of Substances Of Which Semiconductor Devices Are Composed (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP60143189A JPS623092A (ja) | 1985-06-28 | 1985-06-28 | BaPbO3系酸化物超伝導体単結晶の溶液引上げ法による製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP60143189A JPS623092A (ja) | 1985-06-28 | 1985-06-28 | BaPbO3系酸化物超伝導体単結晶の溶液引上げ法による製造方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS623092A true JPS623092A (ja) | 1987-01-09 |
| JPH0243717B2 JPH0243717B2 (fr) | 1990-10-01 |
Family
ID=15332942
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP60143189A Granted JPS623092A (ja) | 1985-06-28 | 1985-06-28 | BaPbO3系酸化物超伝導体単結晶の溶液引上げ法による製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS623092A (fr) |
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US5162297A (en) * | 1987-06-11 | 1992-11-10 | Kabushiki Kaisha Toshiba | Liquid phase epitaxial growth of high temperature superconducting oxide wafer |
| US6094404A (en) * | 1996-01-23 | 2000-07-25 | Seiko Epson Corporation | Display structure with solar cell, and electronic devices and timepiece powered by solar cell |
Families Citing this family (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH03279017A (ja) * | 1990-03-28 | 1991-12-10 | Mazda Motor Corp | 車両のパワートレイン構造 |
-
1985
- 1985-06-28 JP JP60143189A patent/JPS623092A/ja active Granted
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US5162297A (en) * | 1987-06-11 | 1992-11-10 | Kabushiki Kaisha Toshiba | Liquid phase epitaxial growth of high temperature superconducting oxide wafer |
| US6094404A (en) * | 1996-01-23 | 2000-07-25 | Seiko Epson Corporation | Display structure with solar cell, and electronic devices and timepiece powered by solar cell |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0243717B2 (fr) | 1990-10-01 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JPH0152359B2 (fr) | ||
| JPS6345198A (ja) | 多元系結晶の製造方法 | |
| JP2740427B2 (ja) | 酸化物結晶の作製方法 | |
| US3401023A (en) | Crystal melt-growth process wherein the melt surface is covered with an inert liquid | |
| Kozuki et al. | Metastable crystal growth of the low temperature phase of barium metaborate from the melt | |
| Goodrum | Top-seeded flux growth of tetragonal GeO2 | |
| JPH0243717B2 (fr) | ||
| US4708763A (en) | Method of manufacturing bismuth germanate crystals | |
| JPH01249691A (ja) | 超電導薄膜製造法 | |
| US3939252A (en) | Dilithium heptamolybdotetragadolinate | |
| JPS6156200B2 (fr) | ||
| JPS63274695A (ja) | 銅酸ランタン単結晶の製造方法 | |
| JPH0471876B2 (fr) | ||
| JP3936767B2 (ja) | 酸化物結晶の作製法 | |
| JPS63215598A (ja) | 低温相硼酸バリウム単結晶の育成方法 | |
| JP3613424B2 (ja) | 酸化物超電導体の製造方法 | |
| JPS5938197B2 (ja) | 鉛ビスマス酸バリウム単結晶の成長用溶融物 | |
| JPH01148796A (ja) | 酸化物超電導体結晶の製造方法 | |
| JPS63274697A (ja) | 銅酸ランタン単結晶の製造方法 | |
| JP3000137B2 (ja) | 超伝導体PrBa2Cu3Oy単結晶の製造方法 | |
| JP2833640B2 (ja) | Pr123結晶の作製法 | |
| JP2637123B2 (ja) | 酸化物超電導体結晶の製造方法 | |
| JPS5938196B2 (ja) | 鉛ビスマス酸バリウム単結晶の成長方法 | |
| JPH01148794A (ja) | 酸化物超電導体結晶の製造方法 | |
| JPS606913B2 (ja) | ホウ酸インジウム単結晶の製造方法 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| EXPY | Cancellation because of completion of term |